Electronics Forum: alloy 42 sn90 pb10 (2)

0402 tombstoning and dewetting on QFP256 trade-off

Electronics Forum | Thu Mar 12 06:37:48 EDT 2009 | gregoryyork

I agree you are too cold for the profile get it up to 230C and possibly allow it to dwell a little longer in preheat as opposed to pushing up the reflow zone only. Sn90/Pb10 melts at 220C so 2C hotter than your profile so you are reliant on it alloyi

Use of Pb-free Components

Electronics Forum | Fri Mar 19 11:48:06 EST 2004 | Ken

This is the dilema during this transition period. Here is a tip: If you see typcial solder joints on a lead free process, but only on one component type....it probably has a significant quantity of lead in it (ex. Sn90/Pb10...and so on) If using T

Express Newsletter: alloy 42 sn90 pb10 (172)

SMTnet Express - July 1, 2015

SMTnet Express, July 1, 2015, Subscribers: 22,969, Members: Companies: 14,445, Users: 38,464 Reliability Screening of Lower Melting Point Pb-Free Alloys Containing Bi Joseph M. Juarez, Michael Robinson, Joel Heebink; Honeywell International

Impact of Reflowing A Pb-free Solder Alloy Using A Tin/Lead Solder Alloy Reflow Profile On Solder Joint Integrity

Impact of Reflowing A Pb-free Solder Alloy Using A Tin/Lead Solder Alloy Reflow Profile On Solder Joint Integrity If you don't see images, please visit online version at #Application.SmtNet.baseURL#/express/ The Impact of Reflowing A Pb


alloy 42 sn90 pb10 searches for Companies, Equipment, Machines, Suppliers & Information

Sm t t t t t t t t t t net
  1 2 3 4 5 6 7 8 9 10 Next
PCB Handling Machine with CE

High Resolution Fast Speed Industrial Cameras.
Electronics Equipment Consignment

High Throughput Reflow Oven
2024 Eptac IPC Certification Training Schedule

World's Best Reflow Oven Customizable for Unique Applications
Global manufacturing solutions provider

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...


Internet marketing services for manufacturing companies