Re: Poor Solder on TSOP

Electronics Forum | Thu Jun 25 20:26:37 EDT 1998 | Chiakl

| I am looking for a little enlightenment with an issue that we have been seeing. We have SMT assemblies with poor solderability on TSOP and mini-QFP type devices. The solder appears to have incomplete reflow and/or grainyness to the joints. Everythi

Re: Poor Solder on TSOP

Electronics Forum | Tue Jun 30 11:51:41 EDT 1998 | Michael Fogel

| | I am looking for a little enlightenment with an issue that we have been seeing. We have SMT assemblies with poor solderability on TSOP and mini-QFP type devices. The solder appears to have incomplete reflow and/or grainyness to the joints. Everyt

Re: Poor Solder on TSOP

Electronics Forum | Thu Jul 02 19:18:31 EDT 1998 | Rin

| | | | I am looking for a little enlightenment with an issue that we have been seeing. We have SMT assemblies with poor solderability on TSOP and mini-QFP type devices. The solder appears to have incomplete reflow and/or grainyness to the joints. E

Re: Poor Solder on TSOP

Electronics Forum | Thu Jun 25 20:16:01 EDT 1998 | chiakl

| I am looking for a little enlightenment with an issue that we have been seeing. We have SMT assemblies with poor solderability on TSOP and mini-QFP type devices. The solder appears to have incomplete reflow and/or grainyness to the joints. Everythi

BGA Picture Evaluation

Electronics Forum | Wed Apr 09 13:30:20 EDT 2003 | davef

In order to get reliable reflow, you need to be at or higher than [liquidus + 20*C] for about 5 to 10 seconds. [I said 25* in a earlier post, but in an effort to stay on message, I'll stick with 20*] Don't forget that your liquidous is probably NOT

Immersion Gold

Electronics Forum | Sat Jun 26 15:26:10 EDT 2004 | russ

I am very happy with Alpha Metals WS709 or even WS609. Almost all of our product is Immersion gold and we place down to 16mil pitch every day along with 0201 and uBGA. Immersion gold from my experience, solders extremely well with every paste I hav

caps have yellow stain after wash

Electronics Forum | Tue Jun 07 10:24:59 EDT 2016 | davef

wlsmt: You’ve got to help us out here: * Why did you apply solder paste to capacitors prior to water washing the PCBA [where the caps were attached?]? * Did you reflow the Alpha WS-609? * How is the Alpha WS-820 involved in this? * Talk about the

Re: Poor solderability

Electronics Forum | Fri Feb 11 05:44:08 EST 2000 | Dean

Sounds like black pad to me. I just suffered this last week. Track your fab lot codes. Just in case. I processed 1000 fabs of 2 lot codes through 1 line (also WS609). 1 lot code failed with black pad the other did not. With one common mfg. proc

MicroBGA printing problem

Electronics Forum | Mon Sep 20 14:53:24 EDT 1999 | Doug

I've had some trouble pasting a test board for a MicroBGA trial. Most of the paste remains in the stencil apertures. The stencil is 6 mil thick, laser cut and electo-polished. The apertures are 12 mil in diameter with 20 mil pitch. We are using Alpha

Re: Altera PQFP240 Solderability

Electronics Forum | Tue Apr 14 09:01:36 EDT 1998 | Justin Medernach

| We are having some difficulty soldering a 240 pin Altera device. We use Alpha WS-609, a very generic profile for that solder paste, and a 6 mil stencil with laser cut apertures (1:1 ratio). This is a 20 mil pitch device (aperture size is 10 mils X


ws 609 flux searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
PCB Handling with CE

Reflow Soldering 101 Training Course
Solder Paste Dispensing

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
High Throughput Reflow Oven

Training online, at your facility, or at one of our worldwide training centers"
Hot selling SMT spare parts and professional SMT machine solutions

Low-cost, self-paced, online training on electronics manufacturing fundamentals