Electronics Forum | Thu Nov 03 08:34:25 EST 2005 | Slaine
Hi We currently use a small amount of Alloy : 43Sn 43Pb 14Bi Flux: RMA-51AC, Metal : 88.5%. We use it for reworking a product and only consume about 100g per year, we are in the middle or ordering in some more paste but the MOQ is 500g. Is it possibl
Electronics Forum | Wed Jan 15 11:18:51 EST 2020 | avillaro2020
Hi Evtimov, Thanks again! The solder wicking/open solder joint is not actually gross rejection, it is only a few and appeared random (difficult to trend the location of the opens), what is perflexing is that i have this 1 or 2 open solder joints sur
Electronics Forum | Mon Mar 07 09:23:25 EST 2016 | rgduval
We've had our My500 for about four months now, and couldn't be happier. We are a super-high-mix, super-low-volume shop, and the flexibility provided by the 500 over stencils is stunning. So, you buy 5-10 stencils a week? That's 260-520 stencils a
Electronics Forum | Thu May 26 19:32:13 EDT 2005 | Mike Konrad
Three popular methods: Resistivity of Solvent Extract (ROSE) Test Method IPC-TM-650 2.3.25: The ROSE test method is used as a process control tool to detect the presence of bulk ionics. The IPC upper limit is set at 10.0 *g/NaCl/in2. This test is p
Electronics Forum | Wed Oct 03 23:59:44 EDT 2018 | gaintstar
Flason SMT problem solving: http://www.flason-smt.com/new/PRINCIPLE-OF-SURFACE-MOUNT-PROCESS-SMT-PROCESS.html http://www.flason-smt.com/new/Printed-Circuit-Board-PCB-Price-Estimator.html http://www.flason-smt.com/new/Printed-Circuit-Board-Solder-res