Electronics Forum: bga humiseal (Page 1 of 1)

BGA failure after coating

Electronics Forum | Thu Oct 01 03:03:29 EDT 2009 | cunningham

what we are getting is open circuits not every BGA is failing we use Humiseal 1A33 and currently there is no masking instruction for around the BGA

BGA failure after coating

Electronics Forum | Thu Oct 01 07:03:55 EDT 2009 | davef

We doubt that Humiseal 1A33 is causing opens in your assemblies. We'd guess the opens occur earlier in the process, but are not hard failures. So, you pass your tests. When applied, the conformal coat flows into the gap in the ball crack and insulate

Conformal Coat Thermal Conductivity

Electronics Forum | Wed Apr 18 09:16:51 EDT 2007 | Cecil

We currently have an assembly that we have to mask the surface of several (24)SMT components where thermal compound is applied at a latter operation. These component packages vary from BGA's to QFP's. After the thermal compound is applied the PWA is

Humiseal 1A33 conformal coating using automated atomized spray

Electronics Forum | Tue Jul 03 01:54:42 EDT 2018 | rdhiman1

Reaching out to all conformal coating experts, please help! While setting up conformal coating using the automated atomized spray, we observing issues associated with conformal coating wetting on the following regions: 1) Component edges 2) Metalli