Electronics Forum | Fri Dec 10 12:24:46 EST 2010 | davef
Causes of dewetting in conformal coating. Factors that influence dewetting usually involve non-ionic contamination such as: * Residues from board manufacture including silicone surfactants from solder resist & HASL rinse contamination * Component res
Electronics Forum | Tue Jan 10 14:34:40 EST 2006 | Amol Kane
arent there environmentally friendly solvents (i have seen some from 3M) that can be used in a vapor degreaser. i was also planning to use the vapor degreaser to clean boards prior to conformal coating
Electronics Forum | Thu Jan 13 11:12:54 EST 2000 | jacqueline coia
Does anyone conformally coat PCBs that have been processed with a no-clean solder paste? Any comments on this subject would be appreciated. Cheers
Electronics Forum | Fri Jan 14 13:28:13 EST 2000 | DaveH
EMPF is now in Philadelphiaunder the auspices of the American Competitiveness Institute. Ph 610-362-1200 Fax 610-362-1290 www.empf.org
Electronics Forum | Thu Mar 08 01:19:16 EST 2001 | Mike Moninger
The environment essentially defines the need for coating. "Inside" may mean inside a men's locker room with attendant high humidity or inside a climate-controlled clean environment. Conformal coatings offer protection against moisture, fungus, chemi
Electronics Forum | Fri Nov 21 18:56:41 EST 2003 | jsloot
Gun wash is another term used for acrylic laquer thinner. We use DuPont 3642SC. We have much success in its use.
Electronics Forum | Fri Jun 19 15:17:54 EDT 1998 | Chris Jackson
We are in the process of validating Silicon 1C55 (thermal cure) conformal coating over Alpha LR725 solder paste. I am looking for anyone who may be using this process, or has been exposed to someone who is doing this process. Our concern is with the
Electronics Forum | Wed Oct 27 13:20:47 EDT 2004 | DavidB
We are producing boards with Alpha 591S RMA No-Clean paste and are coating after SMC with Dow silicone ( toluene solvent based) conformal coating. We have experienced several failures due to soft shorts ( electrochemical migration?) We have also obse
Electronics Forum | Wed Feb 23 22:38:28 EST 2005 | davef
We: * Cure 1B73 according to spec in a heat box, like a Blue-M * Clean nozzles [one set in use, one set being cleaned] in thinner in a bronson ultrasonic cleaner * Haven't evaluated coatings in years, but would do it according to J-STD-001C, Reqmnts
Electronics Forum | Sat Apr 21 08:26:57 EDT 2007 | Cmiller
Has anyone experienced a problem with conformal coating adhesion to IS-410 boards? We are having problems with one suppliers boards. IS-410 boards from other suppliers are fine and all FR-4 boards that I have looked at are fine. We are using Conap