Nitrogen and dry cabinet

Electronics Forum | Mon Jul 29 21:41:22 EDT 2002 | davef

Rite. Moisture, not N2, in the air is the issue.

Nitrogen and dry cabinet

Electronics Forum | Tue Jul 30 08:38:55 EDT 2002 | dasal

Truthfully, there are pro's and con's for both technologies. (put cost of ownership aside for one moment) Nitrogen won't dry humidified components as rapidly as a desiccant dry box. I'm talking about a self regenerating dry box that uses molecular s

dry solder paste

Electronics Forum | Wed Feb 23 17:24:06 EST 2005 | Austinj

Solder spattering, solder balls, components "popping" off pads........ Not a serious chemical reaction, however, as replied to by KEN on 12/21/04 in a similar article: "Are you adding liquid flux? Or paste "Gel" flux? If liquid flux: This, in my m

Solder Paste not dry after Wave

Electronics Forum | Wed Feb 23 01:06:06 EST 2011 | kemasta

Hi all Recentlt I encounter a issue, the solder paste was not dry after wave. Mostly happen and the end of the board. It is rare case, 1 day happen about twice. But to achieve our quality target, I still need to overcome this issue. I use Alpha OM-

Keeping Blue tooth dry during wash

Electronics Forum | Tue Nov 29 08:03:29 EST 2016 | robl

Is it non washable or non ultrasonic washable? Just asking as there will be some sort of xtal in the module that may have harmonic issues. Worth checking with the manufacturer.

Reflow soldering issue

Electronics Forum | Thu Aug 30 16:17:07 EDT 2018 | emeto

First suspect PCB contamination - clean the boards, bake/dry them, try again.

Unusual solderability issue

Electronics Forum | Fri May 07 00:52:24 EDT 2010 | boardhouse

Hi Derek, just curious of one thing - are the vias within the BGA's the only vias covered or are all vias on the board covered. Just trying to figure out what is making this area different from the rest of the board. Regarding leaching, I do not be

Unusual solderability issue

Electronics Forum | Thu Apr 15 10:05:50 EDT 2010 | dwonch

Hi all, Long story ahead.... We are having issues with board vendors on some of our higher layer count (thick) boards. Specifically under BGAs with high aspect ratio vias (14:1). We are using ENIG finish and a lead free process. Basically we get t

Quad IVc Part rejection issue

Electronics Forum | Sun Sep 09 02:24:04 EDT 2012 | audere

More lube on the O-Rings caused lots of problems. Nozzles would drop downward at times. So I pulled everything out and started from scratch. Testing 3 new Z-Rods, 4 used Z-Rods in good shape (replaced the O-Rings) and around 20 nozzles - the proces

Re: ESD Compliant - Air blow off to dry washed circuit board assemblies

Electronics Forum | Wed Apr 12 21:04:10 EDT 2000 | Dave F

Ashok: You still didn�t tell me why you want additional drying of your boards, but what the hey, we all have our dark secrets. Anywho, let�s consider some options for reducing the moisture of your cleaned boards: OPTION 1 - Up-Grading Your Cleaner

  1 2 3 4 5 6 7 8 9 10 Next

dry issue searches for Companies, Equipment, Machines, Suppliers & Information

2024 Eptac IPC Certification Training Schedule

High Throughput Reflow Oven
Electronics Equipment Consignment

World's Best Reflow Oven Customizable for Unique Applications
pressure curing ovens

We offer SMT Nozzles, feeders and spare parts globally. Find out more
SMT feeders

High Precision Fluid Dispensers