Electronics Forum | Tue Aug 22 08:52:39 EDT 2000 | genesmelik

Good morning Dr. Lee. I was wondering how flux chemistries have changed, or will change, with the transiton to Pb-Free, given the higher reflow temperatures required for SMT assembly?

Water wash flux and cleaning

Electronics Forum | Mon Jun 19 09:47:23 EDT 2017 | georgetruitt

You have a lot to think about! What does the flux manufacturer recommend as far as specifics like water temp or pressure? Do they recommend high temp di-water a detergent or saponifier? Do you currently have a cleaning machine, batch cleaner or inl

flux build up in oven flux filter unit clog

Electronics Forum | Tue Jan 23 23:28:54 EST 2007 | jovial_guy23

If you have flux deposits on the cooling plates, try out Zestron's VIGON RC101...It is an extremely good product especially for reflow ovens and wave solder systems. Check it out...Minimal maintenance water based chemistry with no flash point...Much

Beaker Scale Testing for flux cleaning chemistries/surfactant

Electronics Forum | Fri Apr 22 10:50:51 EDT 2011 | blnorman

Quick question, how are you measuring the effectiveness of the cleaning process to remove the flux?

Removal of No-Clean flux residue

Electronics Forum | Wed Sep 05 17:37:56 EDT 2001 | seand

Hello Jeff, If you have components on your board be careful of how low the frequency is that you will be applying to your board. Ultrasonics are great for cleaning stencils and bare boards at around 40kHz. These frequencies (and Lower)may however

Beaker Scale Testing for flux cleaning chemistries/surfactant

Electronics Forum | Sat Apr 23 00:21:10 EDT 2011 | azrina

As am doing screening right now, am not measuring the total cleanliness yet, i just observe by taking photos (FYI, am varying speed for conveyor belt for cleaning) and see whether the flux is able to be removed by certain parameters. the speed am usi

Beaker Scale Testing for flux cleaning chemistries/surfactant

Electronics Forum | Fri Apr 22 05:01:19 EDT 2011 | azrina

Hi, I am doing my master degree in flux cleaning process for flip chip assemblies and required to establish a new receipt for flux cleaning. currently, i am doing screening process for the parameters involve ; temp,pressure, surfactants, speed and a

Cleaning after rework, no clean flux

Electronics Forum | Wed Feb 26 23:59:48 EST 2003 | Mike Konrad

Grant, No-Clean paste + IPA = White Residue! #1: Stop using IPA #2: Switch to either a solvent-based de-fluxing chemical or an aqueous-based de-fluxing chemical. If you are using an ultrasonic cleaner for your boards as stated, do not use sapon

No-Clean flux residue and RF application

Electronics Forum | Tue Aug 30 15:05:23 EDT 2005 | Shean Dalton

Dear Ing, Have you analyzed why some RF device aren't operational after washing? An assumption is that failures are related to the ultrasonic energy applied. Other possibilities are for poor rinsing, poor drying, inadequate washing on those failed

No-Clean flux residue and RF application

Electronics Forum | Tue Aug 30 12:08:09 EDT 2005 | slthomas

The answer for us at my previous employer was water soluble flux. Wash the board, no residue. If you're not set up to wash (needing a washer, DI water source, waste treatment, ventilation, etc.) it can be expensive and space consuming. Do some resea

  1 2 3 4 5 6 7 8 9 10 Next

flux chemistries searches for Companies, Equipment, Machines, Suppliers & Information

Software for SMT

World's Best Reflow Oven Customizable for Unique Applications
Sell Your Used SMT & Test Equipment

High Precision Fluid Dispensers
Formic Reflow Soldering

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
PCB separator

Internet marketing services for manufacturing companies