Electronics Forum | Mon Sep 21 08:14:14 EDT 1998 | Steve Gregory

| Hello: | I would like to know what causes tombstombing and how can it be prevented? | Thx. | Nichol Hi Nichol! A tombstone happens when solder doesn't wet equally on both terminations during reflow...now why that happens can be found by looking at