Technical Library: solder ball coplanarity (Page 1 of 5)

Vacuum Fluxless Reflow Technology for Fine Pitch First Level Interconnect Bumping Applications

Technical Library | 2023-01-17 17:58:36.0

Heterogeneous integration has become an important performance enabler as high-performance computing (HPC) demands continue to rise. The focus to enable heterogeneous integration scaling is to push interconnect density limit with increased bandwidth and improved power efficiency. Many different advanced packaging architectures have been deployed to increase I/O wire / area density for higher data bandwidth requirements, and to enable more effective die disaggregation. Embedded Multi-die Interconnect Bridge (EMIB) technology is an advanced, cost-effective approach to in-package high density interconnect of heterogeneous chips, providing high density I/O, and controlled electrical interconnect paths between multiple dice in a package. In emerging architectures, it is required to scale down the EMIB die bump pitch in order to further increase the die-to-die (D2D) communication bandwidth. Aa a result, bump pitch scaling poses significant challenges in the plated solder bump reflow process, e.g., bump height / coplanarity control, solder wicking control, and bump void control. It's crucial to ensure a high-quality solder bump reflow process to meet the final product reliability requirements. In this paper, a combined formic acid based fluxless and vacuum assisted reflow process is developed for fine pitch plated solder bumping application. A high-volume production (HVM) ready tool has been developed for this process.

Heller Industries Inc.

THE LAST WILL AND TESTAMENT OF THE BGA VOID

Technical Library | 2023-01-17 17:22:28.0

The impact of voiding on the solder joint integrity of ball grid arrays (BGAs)/chip scale packages (CSPs) can be a topic of lengthy and energetic discussion. Detailed industry investigations have shown that voids have little effect on solder joint integrity unless they fall into specific location/geometry configurations. These investigations have focused on thermal cycle testing at 0°C-100°C, which is typically used to evaluate commercial electronic products. This paper documents an investigation to determine the impact of voids in BGA and CSP components using thermal cycle testing (-55°C to +125°C) in accordance with the IPC- 9701 specification for tin/lead solder alloys. This temperature range is more typical of military and other high performance product use environments. A proposed BGA void requirement revision for the IPC-JSTD-001 specification will be extracted from the results analysis.

Heller Industries Inc.

Surface Insulation Resistance (SIR) Testing

Technical Library | 2007-02-01 09:36:26.0

Purpose: Compare the Surface Insulation Resistance of reworked BGA Test samples made with standard solder balls using a flux only reattachment and samples made including the StencilQuik™ product from Best Inc. with solder balls using a flux only reattachment.

BEST Inc.

New BGA Solder Mask Repair Technique Using Laser Cut Stencils

Technical Library | 2007-02-01 10:08:40.0

The increased replacement of high lead count SMT devices with BGAs and other high ball count area array packages has brought increased challenges to PCB rework and repair. Often solder mask areas surrounding BGA pad areas are damaged when components are removed.

BEST Inc.

BGA Rework. A Comparative Study of Selective Solder Paste Deposition For Area Array Packages

Technical Library | 2007-02-01 09:57:15.0

The rapid assimilation of Ball Grid Array (BGA) and other Area Array Package technology in the electronics industry is due to the fact that this package type allows for a greater I/O count in a smaller area while maintaining a pitch that allows for ease of manufacture.

BEST Inc.

Selective Solder Paste Deposition Reliability Test Results.

Technical Library | 2007-06-21 17:03:16.0

The rapid assimilation of Ball Grid Array (BGA) and other Area Array Package technology in the electronics industry is due to the fact that this package type allows for a greater I/O count in a smaller area while maintaining a pitch that allows for ease of manufacture (...) While there have been several studies comparing these two attachment methods, this study highlights the effect of rework technique on the electrical characteristics and reliability of reworked BGAs.

BEST Inc.

Investigation and Development of Tin-Lead and Lead-Free Solder Pastes to Reduce the Head-In-Pillow Component Soldering Defect.

Technical Library | 2014-03-06 19:04:07.0

Over the last few years, there has been an increase in the rate of Head-in-Pillow component soldering defects which interrupts the merger of the BGA/CSP component solder spheres with the molten solder paste during reflow. The issue has occurred across a broad segment of industries including consumer, telecom and military. There are many reasons for this issue such as warpage issues of the component or board, ball co-planarity issues for BGA/CSP components and non-wetting of the component based on contamination or excessive oxidation of the component coating. The issue has been found to occur not only on lead-free soldered assemblies where the increased soldering temperatures may give rise to increase component/board warpage but also on tin-lead soldered assemblies.

Christopher Associates Inc.

Understanding the Effect of Process Changes and Flux Chemistry on Mid-Chip Solder Balling

Technical Library | 2016-11-30 21:30:50.0

Mid-chip solder balling is a defect typically associated with solder paste exhibiting poor hot slump and/or insufficient wetting during the reflow soldering process, resulting in paste flowing under the component or onto the solder resist. Once molten, this solder is compressed and forced to the side of the component, causing mid-chip solder balling.This paper documents the experimental work performed to further understand the impact on mid-chip solder balling from both the manufacturing process and the flux chemistry.

Henkel Electronic Materials

Stereo Vision Based Automated Solder Ball Height Detection

Technical Library | 2015-04-16 16:11:43.0

Solder ball height inspection is essential to the detection of potential connectivity issues in semi-conductor units. Current ball height inspection tools such as laser profiling, fringe projection and confocal microscopy are expensive, require complicated setup and are slow, which makes them difficult to use in a real-time manufacturing setting. Therefore, a reliable, in-line ball height measurement method is needed for inspecting units undergoing assembly. (...) In this paper, an automatic, stereo vision based, in-line ball height inspection method is presented. The proposed method includes an imaging setup together with a computer vision algorithm for reliable, in-line ball height measurement.

Intel Corporation

A New Stencil Rulebook for Wafer Level Solder Ball Placement using High Accuracy Screen Printing

Technical Library | 2007-12-13 17:03:02.0

Printer-hosted processes for solder ball placement are now widely used for package technologies ranging from BGAs using ball diameters above 750μm to the latest WL-CSPs demanding 250μm diameter. This broadening spectrum of applications brings more choices in terms of stencil design rules and production methodologies.

ASM Assembly Systems (DEK)

  1 2 3 4 5 Next

solder ball coplanarity searches for Companies, Equipment, Machines, Suppliers & Information

Electronics Equipment Consignment

Training online, at your facility, or at one of our worldwide training centers"
Win Source Online Electronic parts

Software for SMT placement & AOI - Free Download.
High Throughput Reflow Oven

Smt Feeder repair service centers in Europe, North, South America
Win Source Online Electronic parts

We offer SMT Nozzles, feeders and spare parts globally. Find out more
SMTAI 2024 - SMTA International

Reflow Soldering 101 Training Course
Electronic Solutions R3

"Heller Korea"