Industry Directory | Manufacturer
Aoki Laboratories Ltd. is an ISO-9002 certified company specializes in manufacturing of Sn/Pb Bar Solder, Cored Wire and Paste.Environmental friendly products, such as: lead-free solder, no-clean non-halide solder flux, no-clean cored wire and Non-CFC cleaner, are compliance with ISO-14001 requirements.
New Equipment | Solder Materials
An alcohol based, halide free, no-clean liquid flux designed specifically to have a very wide process window for wave solder applications.Flux, No Clean Liquid, NC-264-5, (4 Gallon Case)
New Equipment | Solder Materials
Shenmao Technology offers a full line of Water Soluble Fluxes and Water Soluble Solder Paste for SMT and IC packaging applications. We provide halide-containing and halide-free fluxes for Tin/Lead as well as Lead-Free solder alloys. Our formulations,
Electronics Forum | Tue Jun 01 11:51:48 EDT 1999 | Dave F
| We have experienced problems with chlorine damaging certain components, is there anyone with similar problems and possible solutions ? preferably info about a source for chlorine free solder paste | | Thanks | | James | James: There is no chlor
Electronics Forum | Mon Feb 25 14:32:37 EST 2002 | Kelvin
We always talk about the halide free fluxes and solder pastes. Is there anyone tell me what is the industrial acceptable level of halide content or contamination in flux residue? All comment are welcome !!! Kelvin
Industry News | 2011-04-22 21:54:12.0
The Capital Chapter is announcing its next SMTA meeting to be held at APL, Johns Hopkins University, in Laurel MD on May 17, 2011 from 5pm-8pm.
Industry News | 2009-07-16 14:35:03.0
POWAY, CA — July 2009 — EasySpheres LLC features Kester’s 959T no-clean, non-corrosive, halide-free Flux Pen®.
Technical Library | 2023-02-13 18:56:42.0
This paper describes the results of an intensive whisker formation study on Pb-free assemblies with different levels of cleanliness. Thirteen types of as-received surface-mount and pin-through-hole components were cleaned and intentionally contaminated with solutions containing chloride, sulfate, bromide, and nitrate. Then the parts were assembled on double-sided boards that were also cleaned or intentionally contaminated with three fluxes having different halide contents. The assemblies were subjected to high-temperature/high-humidity testing (85_C/85% RH). Periodic examination found that contamination triggered whisker formation on both exposed tin and solder fillets. Whisker occurrence and parameters depending on the type and level of contamination are discussed. Cross-sections were used to assess the metallurgical aspects of whisker formation and the microstructural changes occurring during corrosion.
ALPHA® Telecore XL-825 lead-free cored solder wire minimizes spattering in hand soldering operations, thus reducing circuit board contamination and enhancing worker safety and comfort.
A Review of Test Methods and Classifications for Halogen-Free Soldering Materials A Review of Test Methods and Classifications for Halogen-Free Soldering Materials Over the last few years, there has been an increase in the evaluation and use
| https://pcbasupplies.com/type-4-no-clean-solder-paste/
Type-4 No-Clean Solder Paste, Halogen Free Lead-Free SAC305 Solder Paste - PCBASupplies Login Create Account Contact View My Cart Menu