Electronics Forum | Thu Jan 12 17:35:34 EST 2006 | russ

We use immersion Silver for all of our lead free PCBs. They come in the "silver saver" paper you speak of and we have found that they will tarnish after 7 days in the open enviroment. Even with this tarnish we experienced no reflow problems. We are

tarnishing gold surfaces

Electronics Forum | Wed Nov 10 10:41:57 EST 2010 | esoderberg

subject board fabrication calls for .05 -.125um of gold over 2 - 5 um of nickel. When doing double sided reflow using same profile, parts of the gold are tarnishing and causing test pad failures. any ideas as to the cause?

Industry News: tarnish reflow (2)

Different Techniques for Plating

Industry News | 2018-10-18 11:08:03.0

Different Techniques for Plating

Flason Electronic Co.,limited

Dow Electronic Materials to Showcase Leading Materials for Printed Circuit Board Manufacturing at the IPC APEX EXPO

Industry News | 2011-04-06 13:13:52.0

Dow Electronic Materials will showcase its innovative materials for printed circuit boards (PCBs) at this year’s IPC APEX EXPO. Dow will feature a number of its latest products that are tailored to meet the requirements of increasingly complex circuit boards while delivering ever-higher reliability and consistency. Dow’s next-generation of high quality, cost-effective technologies allow customers to meet future market requirements.

Dow Electronic Materials

Express Newsletter: tarnish reflow (879)


tarnish reflow searches for Companies, Equipment, Machines, Suppliers & Information

Sm t t t t t t t t t t net
  1 2 3 4 5 6 7 8 9 10 Next
Best SMT Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications
best pcb reflow oven

Stencil Printing 101 Training Course
High Throughput Reflow Oven

Wave Soldering 101 Training Course
Win Source Online Electronic parts

Software for SMT placement & AOI - Free Download.