Palladium silver surface finish

Electronics Forum | Fri Aug 13 16:54:20 EDT 2004 | davef

If the terminations on your components are not barrier plated, you must be very careful about the amount of time you stay above liquidous. As you'd expect, longer is not better. The longer you stay at liquidous, the more of the component terminatio