Wave soldering profiling

Electronics Forum | Fri May 07 18:34:55 EDT 2004 | Ron Herbert

Bruce, You didn't mention whether you had checked the specific gravity of the flux. Also, most flux manufacturers recommend getting rid of the flux after 40 hours of use.

solder paste stencil life

Electronics Forum | Sat Dec 15 06:34:54 EST 2012 | sowmya

Normally paste manufacturer specifies stencil life of a paste is 10 hours. the question is, if i run a continuous manufacturing for 40 hours, we will be adding 250 g of paste for every two hours. The addition of 250 g will be mixed with the paste whi

aoi

Electronics Forum | Mon Sep 23 12:44:48 EDT 2002 | daanterstegge

Another issue to look at is the efforts that it takes to become familiar with the machine. Where I work we are also looking into AOI machines, and one of our requirements (based on how simple the vendors say their machines are) is that after no more

Tin Lead Solder Paste

Electronics Forum | Wed Aug 12 17:18:03 EDT 2015 | dyoungquist

Here is our solution: We run the assembly line 40 hours per week and use 500g cartridges of solder. We take 1 cartridge out Monday morning and leave it out until the end of the Friday shift when it is put back into the refrigerator. That means you

MSL control

Electronics Forum | Thu Mar 16 22:19:38 EDT 2017 | deanm

First, reflow does not reset the clock for MSL exposure. The best solution is to run the second side before the exposure time expires. I am curious to know why they must sit for 40 hours. If that cannot be done, then store the assemblies in a dry c

MSL control

Electronics Forum | Wed Mar 15 13:35:40 EDT 2017 | scotceltic

I have a double sided PCBA setup. I have MSL components on both assembly sides. When I run Assy Side one I am within the allotted hours remaining on the MSL component. I then wait 40 hours before running 2nd Assy side. By then the hours on the 1s

Re: Baking PWB's

Electronics Forum | Mon May 24 10:45:04 EDT 1999 | John Thorup

| Can anyone help me with the correct baking cycle for removing moisture for PWB's. These are 10 layer double sided SMT. | | Thank You R. J. Klein Wassink in Soldering in Electronics states - 16 hours @ 105C or 40 hours @ 80C in a ventilated oven

Re: Wave Solder Fixtures: Biting the dust FAST!

Electronics Forum | Tue Sep 15 11:03:41 EDT 1998 | Dave Celestian

| Dave, | Sounds like you have material issues. Been there, done that. Tried 'em all. The best, longest lasting material I've found is called Durostone. It's made by a Roeschling, and most of the big fixture cutting houses now offer it as an option

aoi

Electronics Forum | Mon Sep 23 13:08:47 EDT 2002 | dragonslayr

Daan has made a valid point with regards to expertise and use of a machine. Yet I recognize that with advanced technology, trades must occur. A hghly sophisticated AOI unit can and will help reduce overall cost of production. Therefore, a need to ha

BGA Rework

Electronics Forum | Mon Apr 28 04:02:39 EDT 2003 | chrissieneale

Hey, i'm back from the holiday. Progress on this board is quite good actually, althought the guy who i got to take off and replace all the bga's won't even look me in the eye!! He said he had a really tough job re-doing all the paste. 22 BGA's in a

  1 2 Next

40hours searches for Companies, Equipment, Machines, Suppliers & Information

2024 Eptac IPC Certification Training Schedule

Training online, at your facility, or at one of our worldwide training centers"
Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes

World's Best Reflow Oven Customizable for Unique Applications
Software for SMT

High Resolution Fast Speed Industrial Cameras.
Pillarhouse USA for handload Selective Soldering Needs

High Throughput Reflow Oven


"回流焊炉"