Gold Embrittlement In Lead-Free Solder.

Technical Library | 2014-08-07 15:13:44.0

Gold embrittlement in SnPb solder is a well-known failure mechanism in electronic assembly. To avoid this issue, prior studies have indicated a maximum gold content of three weight percent. This study attempts to provide similar guidance for Pb-free (SAC305) solder. Standard surface mount devices were assembled with SnPb and SAC305 solder onto printed boards with various thicknesses of gold plating. The gold plating included electroless nickel immersion gold (ENIG) and electrolytic gold of 15, 25, 35, and 50 microinches over nickel. These gold thicknesses resulted in weight percentages between 0.4 to 7.0 weight percent.

DfR Solutions

  1  

7..0 searches for Companies, Equipment, Machines, Suppliers & Information

Pillarhouse USA for handload Selective Soldering Needs

High Throughput Reflow Oven
Pillarhouse USA for Selective Soldering Needs

Training online, at your facility, or at one of our worldwide training centers"
Hot selling SMT spare parts and professional SMT machine solutions

Software for SMT placement & AOI - Free Download.
SMT spare parts

"回流焊炉"