Electronics Forum | Wed Jul 28 20:28:26 EDT 1999 | Carlos Palacios
Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into n
Electronics Forum | Fri Aug 16 17:08:07 EDT 2002 | davef
Could be. It does indicate imperfection. * �The component was manufactured and shipped correctly and should not need baking in order to use it.� => Sounds good. Most classes of MSD packaging have a self-life. Lots of times it�s expired before it
Electronics Forum | Sun Mar 20 14:47:29 EDT 2011 | floydf
We are going to be placing BGAs for the first time, and I have some questions. Is it recommended top bake all of the boards and all of the BGAs before production? I have had good luck baking boards that didn't wave solder well. It usually turns out
Electronics Forum | Wed Jul 28 20:56:58 EDT 1999 | Dave F
| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into
Electronics Forum | Thu Jul 29 00:23:45 EDT 1999 | ScottM
| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into
Electronics Forum | Thu Jul 29 12:33:38 EDT 1999 | Wolfgang Busko
| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into
Electronics Forum | Fri May 29 14:34:37 EDT 2020 | huske
BEST Inc offers this type of product for custom shape cutouts. You can buy standard circles and squares from many places. soldertools.net/conformal-coating-tapeshapes-laser-cut-3m-type-401-engineering-cad-work/ solder.net/painters-tape-cus
Electronics Forum | Tue May 19 11:56:59 EDT 2020 | philc
Do you buy in the PCB's from a manufacturer? If so, they may well offer such a service for you. We get quite a few different boards that come with either Kapton tape, or liquid masking already applied.
Electronics Forum | Tue May 19 10:28:51 EDT 2020 | smtmartin100
Hi, Our assembly process involves applying Kapton tape to the back side of our device, a laborious cutting and sticking operation. We are scaling up from "cottage industry" so I'm interested to know if you can buy Kapton shapes on a reel cut to our s
Electronics Forum | Fri Aug 10 15:46:07 EDT 2001 | davef
Probably, but the fabricator of these components can best respond to this question. The need to bake depends on the component design. J-STD-020 and J-STD-033 [as I recall] relate to moisture sensitive components and define 6 classes of moisture sen