Electronics Forum | Thu Jun 07 05:11:42 EDT 2012 | cp38260
Hi, I have pcbs (Duroid/RT 5880) with raw copper, soldered in vapour-phase chamber at 230 degrees Celsius. During soldering, copper gets tarnished. Cleaning with Vigon A250 removes the tarnished layer. Indeed, in the VigonA250 techn. datasheet it is
Electronics Forum | Tue Mar 14 12:56:07 EST 2006 | robhs
Q: Is anyone aware of any solderability issues that may exist when soldering beryllium copper parts (in this case spring contacts) to a PCB using standard Pb63/Sn37 solder paste/wire?
Electronics Forum | Thu Jan 10 13:24:36 EST 2013 | kenkay
What is the thickest internal copper layer we could get in a pcb?
Electronics Forum | Mon Nov 15 14:40:38 EST 1999 | Bob Smith
Hi, I have a problem I've never seen before so I hope someone here can help. A recent batch of PCBs arrived where the copper lands delaminate with a small pull. Normally you have to pull pretty hard and the whole land comes off the substrate. These
Electronics Forum | Tue Apr 24 10:44:05 EDT 2018 | lucianooo
Hi, Uusually for professional PCB factory they can supply "By microscopic slicing" services so that you can make sure the cooper thickness is excatly like you need. If factory is small then usually don't have this services,and normally can not test
Electronics Forum | Sun Sep 09 21:59:36 EDT 2018 | sanneyyu
we are a PCB house, you can add some patterns at breaktabs or board edge, this can help you easily verify copper weight for every circuit layer.
Electronics Forum | Thu May 02 20:56:25 EDT 2002 | clunier
I remember reading a magazine article a few years ago that discused using the copper area of a pcb to transfer heat away from large SMT devices. Does anyone know of this article or something similar that I can obtain. The article covered copper area,
Electronics Forum | Mon Dec 20 07:58:02 EST 1999 | pascal MATHIEU
hello guys ; we are using a fine pitch component(0.65mm) on a thick copper PCB (Cu = 90�m) ; in this case we notice that we are in the process'limits , because the different supplier of the PCB are not able to ensure a good stability of it's process
Electronics Forum | Thu May 09 17:19:28 EDT 2002 | davef
Can�t help you with the article that you read. Other places to start are: * 2221, 7.2 Heat Dissipation Considerations, 7.3 Heat Transfer Techniques, and 8.1.10 Heat Dissipation * 2222, 9.1.2 Thermal Relief In Conductor Planes
Electronics Forum | Wed Nov 23 08:43:48 EST 2022 | charles_nguyen
I am having problem with plated hole-copper spacing. I don't know if the gap between plated hole and copper can meet the capacity of PCB manufacturers. My board have 0.5oz copper weight on outer layer and distance of 0.177MM between plated hole and c
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830