Electronics Forum | Mon May 17 13:21:45 EDT 2021 | SMTA-64387881
PWB Bake out or other elevated temperture processes can cause issues with oxidation of that Nickel layer. The gold porosity can vary from batch to batch, but also process changes can contribute. Are you baking the boards or have previous reflow pro
Electronics Forum | Fri Oct 18 06:33:28 EDT 2002 | johnw
Here's one for you lot, dos anyone have a method or a vendor that can clean the ball's of BGA's of oxides to bring them back to 'new' conditions ? I've got a bathc of components that are fairly old and I get some issues with soldering them which I b
Electronics Forum | Thu Dec 29 10:47:05 EST 2005 | Chris
The paper Dave posted the link for is great. I have to go back and read it in depth. I can build prototypes by wirebonding to ENIG. I can do it on a manual wirebonder but I don't have the patience to do it on a magazine to magazine automatic machi
Electronics Forum | Wed Oct 02 15:20:55 EDT 2002 | Eric
Is there a steadfast rule of thumb for a good solder joint on an Enig Gold board. I come across this number 217C when discussing BGA profiles. Is this a published number? I sure could use a reference. Anybody feedback is appreciated.
Electronics Forum | Tue Jul 03 01:54:42 EDT 2018 | rdhiman1
Reaching out to all conformal coating experts, please help! While setting up conformal coating using the automated atomized spray, we observing issues associated with conformal coating wetting on the following regions: 1) Component edges 2) Metalli
Electronics Forum | Sat Sep 20 11:44:39 EDT 2003 | Gabriele
Few questions: - wich type of C-CGA ? (CAST or CLASP column to ceramic attach) - column pitch ? - column count ? - capped (with lid) ? or capless (c4 die on top)? - PCB board zize and thickness ? - PCB copper finisch ? (OSP,HASL, ENIG, etc) - v
Electronics Forum | Fri May 23 00:16:31 EDT 2014 | edriansyah
Hello all. I need you advice and opinion on my problem with BGA drop off from the boards. Initial defect was ICT fail, but due to some accident, the board fell off, and the BGA just pop out. After some search, I end up to conclude it is a black pad
Electronics Forum | Wed Oct 31 04:37:15 EDT 2007 | aj
Hi, My oven has 5 zones each 12 inches in length , giving a total of 70 inches Heating Zone in total. I am working with a 6 layer PCB ,ENIG Finish. I am using Alpha OM338T no-clean Solder Paste. I am working to a cycle time of 4 to 4.5mins RTS p
Electronics Forum | Wed Dec 22 07:20:21 EST 2010 | piter
HI I used both of solder leveling HASL and ENIG, HASL I can recommended for biger pitch is cheaper solder leveling than ENIG but problem with that solder leveling is during the reflow process HASL isn't flat and during reflow process component move
Electronics Forum | Sat Oct 29 20:29:30 EDT 2016 | adamjs
Posting here because all the threads asking for feedback on it are locked. We have been extremely happy with the 4300 tacky flux for BGA attachment. Not only is it both washable and no-clean (i.e. wash-optional), it was also the only tacky flux tha