| | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and sol
Electronics Forum | Fri May 24 09:19:02 EDT 2019 | davef
http://www.nordsonselect.com. Accel: Cookson created Speedline after purchasing: MPM®, Electrovert®, Accel®, and Camalot®. In 2003, KPS Special Situations Fund II purchased Speedline from Cookson. In, 2007, Illinois Tool Works ITW acquired Speedlin
Electronics Forum | Tue May 26 15:27:36 EDT 1998 | Dave F
| | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and s
Electronics Forum | Tue May 26 20:18:09 EDT 1998 | Justin Medernach
| | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and
Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon
| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a