Electronics Forum | Tue Jul 28 07:02:59 EDT 1998 | smd
Right now we are taping the goldfingers which is effective but also expensive. Also, some tape was leaving yellow marks on the goldfingers. We're trying the so-called goldfinger glove from Steven's Products. It's a very small company (probably one gu
Electronics Forum | Fri Jun 25 01:11:31 EDT 1999 | Vinesh Gandhi
| | | Recently, there has been an upsurge in the Pin Hole/Blow Hole problem in our wave soldering process. We are baking the PCBs for 2 Hrs. at 125 degree C. The Wave Soldering profile seems to be O.K. Still the problem is persistent. Can somebody
Electronics Forum | Fri Sep 08 12:03:24 EDT 2017 | rameshraja
Hi, I need the RF 800 Flux Acid titration procedure and also require EPT of the same to add thinner ( RF 800 additive), i.e we are using the flux rf 800 for our wave soldering process having foam fluxer , after 2 hours we are taking sample from the
Electronics Forum | Fri Dec 08 01:05:33 EST 2006 | Setup Guy
Hi Guru, I have a project to evaluate different kind of Solder Bar and Flux to be used in wave solder(RoSH)machine, to choose in which is the best to be use. What is your best practice to evaluate the Solder Bar and Flux ? Cheers, Setup Guy