Has anyone heard of a no clean paste that can be cleaned in straight DI water ?

Electronics Forum | Fri Jan 26 12:57:34 EST 2018 | aqueous

Sorry to disappoint. No-Clean fluxes are resin-based. They are not soluble in water. Water soluble fluxes are by nature Organic Acid and are soluble in water AND must be cleaned within a short period after reflow as they remain conductive and corrosi

To clean or not to Clean??

Electronics Forum | Sat May 29 16:04:49 EDT 1999 | M Cox

I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a double-sided

Re: To clean or not to Clean??

Electronics Forum | Sun May 30 18:52:35 EDT 1999 | Graham Naisbitt

| | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a

Re: To clean or not to Clean??

Electronics Forum | Sat May 29 16:56:26 EDT 1999 | Jeff Sanchez

| | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a double-

Re: To clean or not to Clean??

Electronics Forum | Sun May 30 10:15:34 EDT 1999 | Vic Lau

| | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a dou

Re: To clean or not to Clean??

Electronics Forum | Mon May 31 21:50:59 EDT 1999 | Dave F

| | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a double-

Re: To clean or not to Clean??

Electronics Forum | Mon May 31 15:09:56 EDT 1999 | JohnW

| | | | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processi

Re: To clean or not to Clean??

Electronics Forum | Mon May 31 15:10:14 EDT 1999 | JohnW

| | | | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processi

Re: When using noclean flux or clean flux process?

Electronics Forum | Wed Sep 22 02:45:23 EDT 1999 | Brian

| | Dear All, | | | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | | | I mean that I wonder

Re: When using noclean flux or clean flux process?

Electronics Forum | Tue Sep 21 13:10:10 EDT 1999 | Dave F

| Dear All, | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | I mean that I wonder why we use