Electronics Forum: selective and carbon and plating (Page 2 of 2)

Foam fluxer maintenance, storage and cleaning

Electronics Forum | Sun Nov 08 15:27:25 EST 2015 | davef

Thinner: Flux thinner, NOT paint thinner We kept a spare stone in thinner in inventory. We cut PVC pipe to size, cap in one end, screw thread on the other, stone inside, filled with flux thinner and covered with a screw cap. I don't remember who we

Gold plated board, with csp's and 0603 with no clean apetures

Electronics Forum | Wed Oct 02 18:18:58 EDT 2002 | davef

The steadfast rule of thumb is: In order to get reliable reflow, you need to be at or higher than [liquidus + 20�C] for about 5 to 10 seconds, rather than those old "60 seconds above 183�C" guideline. This provides for setting your peak based on the