Electronics Forum | Fri Jul 09 18:36:48 EDT 2010 | rway
We don't use flex pcbs but have the same issue here. Most of our pcbs are HASL finish. I have looked at silver and gold immersion and both look really good under my color camera on my AOI. However, gold is more pricey. There is no additional cost
Electronics Forum | Thu Jan 12 10:05:13 EST 2006 | davef
There's a lots comparisons like this on the web. Here's one: Westwood Associates said on 8/12/2003: ||HASL||OSP||ENIG||Pd||Tin||Silver Flat||no||yes||yes||yes||yes||yes Solderjoint||Cu-Sn||Cu-Sn||Ni-Sn||Ni-Sn||Cu-Sn||Cu-Sn Contact||E-test, ICT||no|
Electronics Forum | Fri Aug 10 13:52:58 EDT 2001 | davef
When you say that glue viscosity changes for lot to lot, is this LOT TO LOT of your product OR Loctite�s product? And when you say that glue viscosity changes, what do you mean [eg, increase by � , decrease by � , er watt?]. What specifically is th