Re: Cracking Capacitors and Solder Balls

Electronics Forum | Tue Jun 16 15:00:12 EDT 1998 | Gary Simbulan

There are some common reason for capacitor cracking on my web page if you want to have a look. The document can be downloaded for your reference. | Earl, et al, | Boy things get old and cold around here fast. I promised more detail on my capactior

Re: Cracking Capacitors and Solder Balls

Electronics Forum | Mon Jun 08 15:29:17 EDT 1998 | Gary Simbulan

| Earl, et al, | Boy things get old and cold around here fast. I promised more detail on my capactior problem and I thought I could drop something completely different in the same message and tell a tale of solder balls. | First the caps. We stil

Re: Cracking Capacitors and Solder Balls

Electronics Forum | Tue Jun 16 15:01:58 EDT 1998 | Gary Simbulan

There are some common reason for capacitor cracking on my web page if you want to have a look. The document can be downloaded for your reference. | Earl, et al, | Boy things get old and cold around here fast. I promised more detail on my capactior

Re: Cracking Capacitors and Solder Balls

Electronics Forum | Mon Jun 08 14:52:16 EDT 1998 | Gary Simbulan

| Earl, et al, | Boy things get old and cold around here fast. I promised more detail on my capactior problem and I thought I could drop something completely different in the same message and tell a tale of solder balls. | First the caps. We stil

Inline Aqueous Wash for WS and RMA fluxes

Electronics Forum | Fri Dec 08 02:40:45 EST 2006 | Mike Konrad

Hi 'K', We manufacture both batch and inline defluxing equipment so we have no axe to grind with either technology. There are pros and cons associated with both technologies under specific conditions. Batch machines are typically good cleaners but

Re: Pb alloy reflow temperatures and component integrity

Electronics Forum | Tue Aug 22 16:02:07 EDT 2000 | Dr. Ning-Cheng Lee

If the thermal mass of the products is small, a tent-shaped profile is recommended, with peak temperature around 240C. The hottest spot on board should be less than 250C. However, if the thermal mass of the product is large, such as a large server PC

Step by step guide in evaluation of Solder Bar and Flux

Electronics Forum | Mon Dec 11 20:44:37 EST 2006 | davef

Title : LEAD-FREE WAVE SOLDER FLUX EVALUATION Author : Michael Havener Author Company : Benchmark Electronics, Inc Date : 09/25/2005 Conference : SMTA International Abstract : The European Union�s deadline to ban lead in electronic pr

Previous 1 2  

temperature and cycle and chamber searches for Companies, Equipment, Machines, Suppliers & Information

Fluid Dispensing, Staking, TIM, Solder Paste

Training online, at your facility, or at one of our worldwide training centers"
Electronic Solutions

Easily dispense fine pitch components with ±25µm positioning accuracy.
Global manufacturing solutions provider

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
design with ease with Win Source obselete parts and supplies

Private label coffee for your company - your logo & message on each bag!