Electronics Forum | Thu Mar 13 14:12:31 EDT 2014 | davef
You're creating a new alloy on the surface of your board. The alloy will have a melting point determined by the constituent metals of the alloy. Your alloy consists of: * Lead-free HASL solderability protection on the board * Lead-free solder paste *
Electronics Forum | Mon Feb 01 04:57:08 EST 2016 | oxygensmd
If you can use the standalone mode then choose the program on "option" and somewhere you can load program - "aktuell". The "aktuell" program is the last program what was downloaded on this machine. In SiTest you can test and calibrate the machine. Y
Electronics Forum | Wed Mar 10 13:53:13 EST 1999 | Vincent Vega
| We will wave solder a board with SOIC14 and SOIC16 parts on the bottom. It has been difficult to find any specific wave solder process recommendations from manufacturers of the SOICs. The pad geometry utilizes theiving pads on both sides to reduce
Electronics Forum | Fri Dec 18 12:14:10 EST 1998 | Brian Steelglove
| | Does anyone out there have one we are currently looking at one from a used equipment dealer and would like to know how they work? Good or bad for SMT? | | Good or bad for high volume Thrue Hole? | | | | Thanks Again, | | Brian Steelglove | | A
Electronics Forum | Sat Mar 18 02:21:31 EST 2006 | pavel_murtishev
Good morning, Once again a met annoying solder beading issue while producing board with PLL (leadless, contacts from the bottom side of the package). Board has very high placement density and beads appear near PLL package only. This package is finep
Electronics Forum | Mon Dec 21 08:49:29 EST 1998 | Aric Parr
I used one on SMT at a previous employer. Make sure that you have 3 zones of preheat. Make sure that your operators are trained. The airknifes are extremely difficult to set up properly. Don't use them on high mix lines. We didn't need them once
Electronics Forum | Tue Dec 22 10:00:31 EST 1998 | Chrys
| | | Does anyone out there have one we are currently looking at one from a used equipment dealer and would like to know how they work? Good or bad for SMT? | | | Good or bad for high volume Thrue Hole? | | | | | | Thanks Again, | | | Brian Steelg
Electronics Forum | Thu May 09 17:07:56 EDT 2002 | davef
Troubles, troubles, troubles. If it weren�t for bad luck, I wouldn't no luck at all, eh? Tough business. Comments on your trouble are: * On machine vision errors from less than ideal capacitors: This is life. Reprogram your machine to either wid