Electronics Forum: laminates (Page 2 of 48)

PCB laminate dielectric absorption

Electronics Forum | Wed Dec 13 13:42:57 EST 2000 | Mike Ihm

The dielectic absorption characteristic of printed circuit board materials is usually not listed on the manufacturers spec. sheets. Can anyone point me in a direction to help determine which laminate materials might exhibit better dielectric absorpt

Re: Non-halogenated PCB

Electronics Forum | Wed Jul 19 20:30:38 EDT 2000 | Dave F

Lennart: I think most laminators offer a halide free laminate. Two are Isola and Mica-Micanite. Contact the IPC Halogen-Free Materials Task Group

Laminate base material

Electronics Forum | Sun Mar 26 19:54:47 EST 2000 | Marc

when would one use a difunctional base laminate material as a possed to a tetrafunctional base material? What possible problems are associated with each?

Boards delaminated after wash

Electronics Forum | Tue Aug 14 15:45:06 EDT 2001 | davef

BOARD BAKING SCHEDULE: Bake time depends on the board thickness and construction. For laminated FR4 PCB, we bake between 6 and 24 hours at 100�C. ROOT CAUSE OF THE PROBLEM: Heating moisture entrapped between the laminations of the board too quickl

force between the pad and laminate material

Electronics Forum | Tue Jun 11 22:06:06 EDT 2002 | scottxiao

I encounter the problem, it is easy for pad(copper) to drop off from the PCB, which is Ni/Au finish. so my question is whether there is any specification about the force between pad and laminate material, and does the PCB corpoartion test this parame

Micro BGA pads, adhesion to laminate

Electronics Forum | Wed Jul 09 16:12:01 EDT 2003 | Matt Kehoe

Right-o Dave, Thats the 2 lifted pads turned upside down so actually you are looking at the bottom of the base copper where it used to be attached to the laminate. mk

PCB Material

Electronics Forum | Wed Dec 22 11:12:33 EST 2004 | Steve

Does anyone have an opinion about the pro's and con's of Getek vs Isola FR408 laminate? What laminate to most of you call out? Thanks in advance for your feedback. Steve

The story so far!

Electronics Forum | Thu Dec 07 20:55:08 EST 2006 | Cmiller

Implemented 6 months ago and have noticed no difference in frequency of farting. Sorry, could not resist. Have seen delamination problem with IS-410 laminate. What laminate is everyone else using?

Water Absorption of PCB

Electronics Forum | Thu Feb 15 22:55:45 EST 2007 | davef

Questions are: * Is the blistering in the solder mask or the laminate? * If the blistering is in the solder mask, what do the blisters look like [eg, size, quantity, distribution, etc]? * If the blistering is in the laminate, what do the blisters loo

Td and Tg

Electronics Forum | Wed Aug 27 13:08:30 EDT 2008 | vladig

Td - is the degradation temperature for a laminate (board), while Tg - is glass transition one. There is one more (even more important) - delta Tg. They characterize the quality of the laminate material. Regards, Vlad www.sentec.ca


laminates searches for Companies, Equipment, Machines, Suppliers & Information

Selective soldering solutions with Jade soldering machine

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
Selective soldering solutions with Jade soldering machine

Benchtop Fluid Dispenser
Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes

Best Reflow Oven
PCB separator

Find a wide selection of nozzles, solder materials, storage solutions and more at SALESCON