Electronics Forum | Wed Mar 17 02:14:39 EST 1999 | Joe
| | We are having a small number (~2%) of our boards pass our manufacturing diagnostics, fail once they reach the customer, fail when they get back to us and then start working again after handling them for a short time. We have eliminated a lot of
Electronics Forum | Wed Mar 17 19:00:14 EST 1999 | Earl Moon
| | | We are having a small number (~2%) of our boards pass our manufacturing diagnostics, fail once they reach the customer, fail when they get back to us and then start working again after handling them for a short time. We have eliminated a lot o
Electronics Forum | Wed Jan 17 20:48:14 EST 2001 | davef
We find that the raw BGA's pad sheared surface has the SnPb solder at various Z heights whereas the assembled BGAs pad leave a smooth layer of SnPb along the pad. Like to understand the cause for the difference. Who could guess? Solder joint streng
Electronics Forum | Fri May 15 17:31:04 EDT 1998 | Steve Abrahamson
| | | | We had some failures on an IC package that the manufacturer has put down to moisture inside the package, leading to popcorning. | | | | This seems a bit odd, the package is a PLCC 84 which is quite thick. I have only seen this problem on thin