Electronics Forum | Wed Oct 26 08:26:07 EDT 2011 | edmaya33
Anybody here with extensive knowledge with PVA650/2400SF coating robot? I wanted to know the semi perfect settings for my FCS-300 valves. Anybody can share their thoughts. Tank Pressure: Atomized Pressure: Path Speed: Path Distance: Height: Valve op
Electronics Forum | Fri Feb 02 08:36:14 EST 2007 | CK Flip
Wow, I cut first cut my teeth in the Industrial motor control industry. My 1st company made motor control products like variable speed drives, solid state overload relays, soft starts, etc. and in our shop, we used nothing BUT Dow Corning silicone p
Electronics Forum | Fri Nov 04 13:24:30 EDT 2011 | tombstonesmt
Peelable masking has been our solution here recently. We an automovite customer that requires coating on both sides of the boards with many keep out areas. We are currently building a dispense robot that will apply tech spray wondermask 2218. The won
Electronics Forum | Wed Nov 23 17:50:40 EST 2005 | adlsmt
I am not aware of any such info so you may not get any replys on this but each of these systems is totally different. There is usually not much overlap of what is the right choice for an application. The solder bath machines with fixtures are for hig
Electronics Forum | Wed Feb 23 11:02:41 EST 2000 | John
John, I'll try to take a crack at it. We manufacture our own boards, and have a high mix. We currently have BOTH a Camalot 2800 Dispenser and a DEK 260 Screen printer. We use the camalot for glue applications, and prototype paste. We use the printe
Electronics Forum | Wed Feb 23 11:02:41 EST 2000 | John
John, I'll try to take a crack at it. We manufacture our own boards, and have a high mix. We currently have BOTH a Camalot 2800 Dispenser and a DEK 260 Screen printer. We use the camalot for glue applications, and prototype paste. We use the printe
Electronics Forum | Thu Mar 22 17:37:06 EST 2001 | davef
Hey!!! Watch it!!! I don�t want to get you believing too much of this stuff. But if you bought that, listen to this � some circuits are so critical with that skin effect stuff that they use silver as the top level solderability preservative. Turn
Electronics Forum | Thu Jun 25 14:45:55 EDT 1998 | Chrys
| I have a single-sided board with test vias that pass through the board. The test vias are pasted and reflowed with the SMT components on the top side. When the boards are wavesoldered, the solder coverage on the vias is spotty. Some will sold
Electronics Forum | Thu Dec 22 10:51:12 EST 2005 | killer1994
Yes, I have been using it for 4 years now. We have the 4 axis, 3 head, 2 lines. Inspection station and ir oven. I have to say you will NOT get better support anywhere in this industry than from PVA. Their crew is top notch, always going above and bey
Electronics Forum | Thu Jul 20 17:01:26 EDT 2000 | Bob Willis
Here is some further information on SDSRS process, but please purchase a copy of the report from t he SMTA as all the money goes to charity. In the UK the SMART Group raised over �3000 for the homeless. SMTA have been raising a lot of money for the G