Gold Leaded SMT devices

Electronics Forum | Tue Sep 09 20:32:10 EDT 2003 | davef

The maximum ratio of gold weight to solder alloy weight can be calculated, to help prevent a problem from excessive gold-tin intermetallic compound (i.e., AuSn4). For the equation and its derivation, please refer to "The Use of Capillary Action Measu

Re: Soldering to Gold

Electronics Forum | Fri Sep 17 15:01:05 EDT 1999 | Dave F

| | We have some SMT components with gold plated leads. They're actually LCC led packages. A good solder alloy to use would be Indium / Lead to reduce tin dissolution into the gold and avoid the resultant brittle intermetallic compound. However, a re

Re: Soldering to Gold

Electronics Forum | Sat Sep 18 04:42:52 EDT 1999 | Brian

Dave, I'll respond by paragraph: | | | Brian: | | I like Ag2 also. I prefer it over both 63/37 and 60/40, if the price is not a factor. Yes, gold rips through eutectic and near-eutectic solders like habanero slathered shiitake burritos through

Re: Soldering to Gold

Electronics Forum | Sat Sep 18 12:27:21 EDT 1999 | Earl Moon

| | | Dave, I'll respond by paragraph: | | | | | Brian: | | | | I like Ag2 also. I prefer it over both 63/37 and 60/40, if the price is not a factor. Yes, gold rips through eutectic and near-eutectic solders like habanero slathered shiitake

Problems with TI DSP modules

Electronics Forum | Wed Oct 24 18:08:02 EDT 2001 | davef

1- DF1: WOW!!! How do people get these cool toys? CB: I am with the University at Buffalo Electronic Packaging Lab. http://www.packaging.buffalo.edu We have pretty much everything that is sold on the market as well as Laser inspection technologies we

Re: Soldering to Gold

Electronics Forum | Sat Sep 18 13:05:57 EDT 1999 | Brian

| | | | | | Dave, I'll respond by paragraph: | | | | | | | Brian: | | | | | | I like Ag2 also. I prefer it over both 63/37 and 60/40, if the price is not a factor. Yes, gold rips through eutectic and near-eutectic solders like habanero slath

Re: Soldering to Gold

Electronics Forum | Sat Sep 18 14:37:00 EDT 1999 | Earl Moon

| | | | | | | | | Dave, I'll respond by paragraph: | | | | | | | | | Brian: | | | | | | | | I like Ag2 also. I prefer it over both 63/37 and 60/40, if the price is not a factor. Yes, gold rips through eutectic and near-eutectic solders like

Re: Tinning gold plated leads ( DIP, etc)

Electronics Forum | Tue Mar 21 20:25:30 EST 2000 | Dave F

John: What�s the matter? Free gold � good thing for you, bad thing for your supplier. :^) Pre-tinning of gold plated leads is important to: � Prevent gold embrittlement of the solder joint � Determine if the leads are solderable prior to assembly (