Parylene coating - spots defect around via holes & other flat surface

Electronics Forum | Fri Oct 07 08:48:45 EDT 2016 | davef

Two things ... A friend in the contract coating business said: "... the board is not being baked out long enough, 30 min is certainly not long enough depending on how many layers this board is, as the vacuum (from the parylene process) is pulling t

Re: Moisture Sensitivity and Package Cracking

Electronics Forum | Tue Feb 02 11:07:36 EST 1999 | justin.medernach@flextronics.com

| Greetings, | | We are discussing what should and what should not be baked and vacuum packed. Should we just concentrate on the fine pitch packages and the bga's? | What about those components which come on blister tape, should they get baked and r

Re: Moisture Sensitivity and Package Cracking

Electronics Forum | Mon Jan 25 21:14:08 EST 1999 | Dave F

| Greetings, | | We are discussing what should and what should not be baked and vacuum packed. Should we just concentrate on the fine pitch packages and the bga's? | What about those components which come on blister tape, should they get baked and r

BGA Baking & Tape and Reel Issue

Electronics Forum | Tue Sep 14 07:54:05 EDT 2004 | modwyer

Folks, At the moment I bake all BGA that are in unsealed trays, to reduce moisture etc. Is this common practice or are there particular manufacturuers that cause more problems. Also, the tape for BGA tape & reel has a hole in the tape (as is normal

Percentage of Blowholes and Pinholes can eliminate.

Electronics Forum | Thu Oct 17 05:16:44 EDT 2013 | vincentdesilva2003

Anyone can help me how many percentage of blowholes and pinholes if i do the followings: 1. Increase copper plating thickness more than 25 microns. 2. Pre Baking of PCB to remove gassing by drying out the PCB's

Re: Moisture Sensitivity and Package Cracking

Electronics Forum | Mon Feb 01 10:06:51 EST 1999 | Chris Fontaine

All of our moisture sensitive components are shipped to us in vacuum sealed, desiccated bags with a moisture indicator. When the parts are removed from the bag (this is done at either SMT setup, or in the stockroom) the indicator is checked. If it

Wash and bake of blank PCB's before assembly

Electronics Forum | Thu Jun 04 14:30:13 EDT 1998 | Igmar

I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards before assembly. + Is it necessary to wash and bake PCB�s before assembly? + If any, what is the reason for wash and bake of PCB�s? + If any, what type of

Wash and bake of blank PCB's before assembly

Electronics Forum | Thu Feb 12 16:50:40 EST 1998 | Igmar

I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards before assembly. + Is it necessary to wash and bake PCB�s before assembly? + If any, what is the reason for wash and bake of PCB�s? + If any, what type of

BGA Baking & Tape and Reel Issue

Electronics Forum | Thu Sep 16 21:11:10 EDT 2004 | davef

Left to its own devices the plastic used to seal your parts will take-on moisture in the air. When you heat there parts the water in the part expands and can damage the part, if not properly demoisturized. The instustry standards for controlling su

Electronic Assembly - PCB cleansing and COVID-19

Electronics Forum | Mon Mar 30 13:14:41 EDT 2020 | dwl

Heat above 53 Celsius kills covid viruses according to the WHO: https://www.who.int/csr/sars/survival_2003_05_04/en/ If you want an added measure of safety, you could bake your boards before packing them. Fundamentally its going to be an issue of