Electronics Forum | Thu Oct 01 07:03:55 EDT 2009 | davef
We doubt that Humiseal 1A33 is causing opens in your assemblies. We'd guess the opens occur earlier in the process, but are not hard failures. So, you pass your tests. When applied, the conformal coat flows into the gap in the ball crack and insulate
Electronics Forum | Thu Nov 23 23:59:25 EST 2000 | terry sun
Hello to all out there, We're considering CC process,and would like to know some defferences between SSC3 of Electrolube and Humiseal 1B73, yes,I know that SSC3 is silicone one,and Humiseal 1B73 is solvent based acrylic as well as other basic propert
Electronics Forum | Tue Mar 10 22:16:56 EST 1998 | Steve Gregory
Jeremy, I'm gonna make a couple of assumptions by "reading in between the lines" of your email: 1. You're using no-clean paste. 2. This is only happening on the second side. You tell me if I'm wrong about this... First thing, if you're only experienc
Electronics Forum | Wed Dec 09 08:45:31 EST 2009 | orlando
Does anybody run conformal coating process using UV cure varnish? We have a long experience on solvented urethane coating material but switching to solventless is unknown for us. Could you recommand vendors for UV curing oven? Thanks
Electronics Forum | Mon Apr 08 14:16:29 EDT 2019 | sever_83
We've never heard of seen of such a thing either. We tried a clean sample board and applied con coat. Same process through out and we saw nothing. After speaking with the original operators who was curing the boards he had left the boards much longer
Electronics Forum | Thu Dec 10 15:33:55 EST 2009 | duso02
We use one quite often. Our machine is a Uvitron Conveyor 40 as we are a large coating house and this allows us to process many boards. Dymax also maufactures and sells machines as well. Humiseal and Dymax both manufacture UV coatings. Emerson Cuming
Electronics Forum | Fri Jun 03 14:31:33 EDT 2005 | Peter
I am working on an application requiring removing BGAs from a board coated with parylene. These BGAs have low standoff with less than 0.015" after SMT soldering. Can some comment on a reliable and consistent process to perform such rework? given tha
Electronics Forum | Tue Feb 08 14:23:47 EST 2011 | dennisfo
Conformal coat bubbles using 1B73 and SC-205 nozzle I've read most of the posts on this subject. I'm using the SC-205 (airless) fan nozzle and 400 needle to apply 1B73 mixed with xylene thinner. I have micro bubbles which come directly out of the noz
Electronics Forum | Mon Jun 13 07:44:15 EDT 2005 | bandjwet
Peter: Based on our company's experience with removing a variety of different coatings, including parylene, the BGA's can be removed. We would use a chemical etch followed by a neutralizing process. We would then reflow the devices and pry them off
Electronics Forum | Tue Oct 16 10:06:41 EDT 2018 | emeto