Electronics Forum | Tue May 25 07:19:13 EDT 2010 | jry74
I tried these and the operators didn't like them. The palm dip didn't slide well on tape and the finger tips were a bit bulky.
Electronics Forum | Thu May 20 11:36:57 EDT 2010 | davef
Ansell ANS 11-100 HYFLEX (ESD) static dissipative coated Size||Ansell p/n||Techni-Tool p/n 7||ANS111007||328PR107 8||ANS111008||328PR108 9||ANS111009||328PR109 10||ANS1110010||328PR110
Electronics Forum | Thu Jul 21 16:05:24 EDT 2005 | russ
This is kind of odd, I am accustomed to the Q.C. dept. verifying that criterias/specs have been met per engineering and contractual requirements and not identifying or implementing these specs. I believe that this philosophy aids in eliminating the "
Electronics Forum | Wed May 19 19:41:12 EDT 2010 | jry74
Our employees use a knit style ESD glove when masking boards to prevent oils. They snag alot and bend leads and cause other problems. I have tried dipped palm but they are bulky and dont offer "feel". I tried a silky type but they had a huge seam
Electronics Forum | Tue May 25 12:17:44 EDT 2010 | markhoch
Dang, you're picky. Try buying your operators mittens, and then tell them that your company has discovered that mittens generate less ESD so they're making them mandatory now. Then...after a few hours, bring them their gloves back and tell them that
Electronics Forum | Fri Jan 26 13:26:30 EST 2007 | rw
We are developing a new product that requires conformal coating on the motor controller. We selected a silicone based conformal coat due to its ease of use. There has been disagreement among engineers as to its impact on the motor. We have contact
Electronics Forum | Wed Feb 28 20:10:08 EST 2001 | mhunter
Checked the archives with no luck. Anyone have a reliable test method of verifying acrylic conformal coat cure. Using Humiseal 1B31 mixed with approximately 30% solvent, spraying with a Nordson. Thanks in advance.
Electronics Forum | Wed Feb 28 20:16:26 EST 2001 | mhunter
Checked the archives with no luck. Anyone have a reliable test method of verifying acrylic conformal coat cure. Using Humiseal 1B31 mixed with approximately 30% solvent, spraying with a Nordson. Thanks in advance.
Electronics Forum | Wed Apr 19 11:18:46 EDT 2006 | BJ
Is there a preferred/efficient method(s)(e.g. tape/masking compounds, boots etc.) for masking off specific areas and/or components on a pwb prior to conformal coating?
Electronics Forum | Wed Apr 19 16:24:11 EDT 2006 | patrickbruneel
Here's an other option called seal and peel http://www.interfluxusa.com/misc.html