Electronics Forum | Thu May 18 16:10:18 EDT 2006 | adlsmt
We did a tin bath on ours but it was provided for free by Nihon Superior so that is a no-brainer. It was better than taking a risk of having to dump the pot. If you cant get a free tin bath, then you should probably go ahead and fill it half way or s
Electronics Forum | Mon Nov 05 00:51:58 EST 2007 | omidjuve
We have a problem with soldering of a 96 pin header connector(9001-11961c00l1a from kingmate) we use 3 different wave soldering but in all of the machines we have many short circuit between the pins . the wave soldering machines that we use is fr
Electronics Forum | Thu Apr 04 09:45:58 EDT 2019 | davef
That's what I guessed. Some ideas to consider are: Reduce usage of flux to the bare minimum. Choose a low solids flux Flux residues can be categorized as soft, brittle, sticky but this depends mostly on the formulation of the flux and the resins