Electronics Forum | Fri Feb 02 16:43:15 EST 2007 | Machinebuilder
Can I have a website or email please? Thanks
Electronics Forum | Tue Aug 17 03:03:56 EDT 2004 | soease
thank you Grant and dreamsniper for these shared experiences; I think I'll still try some vapor phase just to have a look to this process, but will focus on a convection as long as it's the actually chosen technology in the company and that it's expe
Electronics Forum | Fri Feb 02 17:39:27 EST 2007 | davef
Machinebuilder: Click on the link just to the right of "Author:" [John Smith] in the response to your quiry in order to email the responder.
Electronics Forum | Fri Feb 09 17:27:59 EST 2007 | stockley
Nice try John, why don't you post them on Equipment Mart and put us all out of our misery.
Electronics Forum | Mon Feb 12 06:02:14 EST 2007 | mk
I think Mark may be able to help you out. Mark Strickland Marshal Space Flight Center MFSC Huntsville AL PO Box 707 MS K68 Huntsville, AL 35812 256-544-7432 mk
Electronics Forum | Mon Feb 12 12:07:19 EST 2007 | john_smith
Brian, I would love to post them on equipment mart but do you really think they would sell?
Electronics Forum | Mon Aug 16 20:19:10 EDT 2004 | Grant
Hi, We have both Vapor Phase ASSCON semi auto as well as Soltec convection inline ovens. I must say we had no end of problems with Vapor Phase. We tried everything, and just could not totally eliminate tomb-stoning completely. We would always get a
Electronics Forum | Tue Feb 24 16:44:55 EST 2009 | ldavis
Yes, we are only running no-clean pastes.
Electronics Forum | Mon Feb 23 14:44:08 EST 2009 | sunny
Are boards produced using Vapor phase ovens dirtier than N2 Reflow oven. Are there any studies/papers someone can point to? if not what are the methods to verify this? is IPC specified SIR test using 24B SIR test coupons? please advise. thanks in adv
Electronics Forum | Tue Aug 18 10:11:04 EDT 2009 | grantp
Hi, Yes, I think this sounds like a form of tomb-stoning, and we used vapor phase until it ended up driving us totally nuts trying to deal with tomb-stoning. We tried everything, and all kinds of stencil apertures. Vapor phase is an amazing process