ENIG used with stainless-steel membrane switch

Electronics Forum | Thu Jul 24 22:58:13 EDT 2008 | davef

At the 2004 IMAPS Nordic Conference, Claus W�rtz Nielsson from Nokia Mobile Phones published "The Evolution of Surface Finishes in Mobile Phone Applications" [www.imaps.org/adv_micro/papers/Nordic2004paper.pdf]. Some of the results were: * Corrosion

Latent shorts on QFN package

Electronics Forum | Fri Mar 06 19:58:59 EST 2009 | macisaint

ENIG

ENIG CONTAMINATION

Electronics Forum | Wed Nov 04 10:01:00 EST 2009 | gregoryyork

10% Wt

ENIG CONTAMINATION

Electronics Forum | Thu Nov 05 04:17:26 EST 2009 | gregoryyork

I see thanks for that

PCB Design Question - Hard gold or ENIG for keypad button contacts

Electronics Forum | Tue Feb 21 03:20:57 EST 2017 | pcbcart

We're a custom PCB manufacturing services provider based in China and we have made many high quality circuit boards for high end products. Based on your project requirements and our years' experience, we are positive that ENIG is totally sufficient.

Immersion Au and ENIG surface finishes

Electronics Forum | Thu May 02 07:11:10 EDT 2002 | davef

They probably the same. Most likely someone is saying immersion gold [immersion Au] as a short hand for ENIG [ Electroless Nickel - Immersion Gold]. It is very uncommon to plate gold directly on copper, because gold and copper form a brittle interm

Gold plated PCB's

Electronics Forum | Thu May 09 15:56:33 EDT 2002 | stownsend

We are using NC. Paste doesn't seem to have an effect on the solderability on a bad batch of ENIG. When ENIG has gone bad, throw the board out.

Bga replacement on ENIG Fabs.

Electronics Forum | Mon Jul 28 16:32:45 EDT 2003 | itempea

Mant, we are reliably replacing BGAs of all sizes and pitches on ENIG. The black pad is not something created through rework, but a defect that the PCB has from the very beginning. Ioan

HIC turn Pink for PCB-URGENT

Electronics Forum | Tue Jul 06 08:04:01 EDT 2004 | ANDREW

Thanks Dave, The surface finish is ENIG.Is it ok not to bake even though the HIC has changed color? What is the shelf life for ENIG boards?

Steam Aging of ENIG

Electronics Forum | Wed Dec 15 10:48:23 EST 2004 | gopinath A

I heard that Steam Aging (storage) tests would be inappropriate for gold finishes. Is this a correct statement? If so, what are the reasons? How bad is the shelf life of ENIG


enig searches for Companies, Equipment, Machines, Suppliers & Information