Electronics Forum | Wed Nov 01 22:58:31 EST 2006 | davef
Durastone is commonly used in flooring. Durostone is a proprietary product of R�chling Permali Composites SA [be aware this is a French company] that many use for reflow and SMT process pallets. Suppliers are: * R�chling Permali Composites SA; Canog
Electronics Forum | Fri Jul 02 05:28:13 EDT 1999 | Vinesh gandhi
| | | We are wave soldering some fabs with a lot of unmasked trace area along the edges. The trace area is solid copper covered with tin / lead, no masking, no components along the edges, same on solder side and component side (goofy board design).
Electronics Forum | Fri Jul 02 09:54:02 EDT 1999 | John Thorup
| | | | We are wave soldering some fabs with a lot of unmasked trace area along the edges. The trace area is solid copper covered with tin / lead, no masking, no components along the edges, same on solder side and component side (goofy board design)
Electronics Forum | Fri Jul 02 10:06:17 EDT 1999 | John Thorup
| | | | We are wave soldering some fabs with a lot of unmasked trace area along the edges. The trace area is solid copper covered with tin / lead, no masking, no components along the edges, same on solder side and component side (goofy board design)
Electronics Forum | Mon May 14 22:24:11 EDT 2001 | davef
The time over liquidous of the profile seems short. But then again, who knows? Based on what you told us, I'm guessing at a board fabrication problem, either measling or delamination. Probably the former, rather than the latter. [Now, we remember
Electronics Forum | Tue Jul 28 07:02:59 EDT 1998 | smd
Right now we are taping the goldfingers which is effective but also expensive. Also, some tape was leaving yellow marks on the goldfingers. We're trying the so-called goldfinger glove from Steven's Products. It's a very small company (probably one gu
Electronics Forum | Mon Aug 03 08:29:24 EDT 1998 | Dave F
SMD: Sounds interesting. What is the contact information on Steve? Dave F | Right now we are taping the goldfingers which is | effective but also expensive. Also, some tape was leaving yellow marks on the goldfingers. We're trying the so-called go
Electronics Forum | Mon Aug 03 08:23:37 EDT 1998 | smd
Stevens Products (supposedly around since 1937) 128 N. Park St. E. Orange, NJ 07019 Tel 973-672-2140 Contact: Ross Stevens, Jr. They'll take a PO but terms are net 30 Right now we are taping the goldfingers which is | effective but also expensive. A
Electronics Forum | Wed Mar 25 14:05:18 EST 1998 | Justin Medernach
| We currently use an abrasive fiberglass brush to clean the silver oxide off of our substrates proir to asembly. It's messy and tiring. Is there an alternative method, either chemical or mechanical that is cost effective for small (30 to 50ea 6in
Electronics Forum | Mon Nov 05 20:34:03 EST 2001 | davef
What�s the problem? There area many heat related failure mechanisms in bare boards. You can damage boards with heat several ways. A couple favorites [Don�t try this at home. Perform on a closed track by professional solders only.] are: * Put a