Electronics Forum | Thu Aug 01 07:06:28 EDT 2002 | gdstanton
Just exploring options to improve wetting. It turns out our facilities dept is looking at an N2 generator to supply dry boxes. Thought it might be a good idea to assess whether we should expand the project to include reflow.
Electronics Forum | Wed Jul 31 14:08:22 EDT 2002 | Dave G
Used this paste on ENIG boards W/O N2 and had very good results. (0402's,BGA's,16mil FP) Never had the need to use N2 with this paste on our products. Running with N2 shouldn't hurt anything. The wetting properties should get even better than they ar
Electronics Forum | Tue May 29 09:36:24 EDT 2007 | davef
oxygen sensor instrumentation Amoung the oxygen monitor suppliers that tailor themselves to reflow machines are: * MapCheck 9000 Process Oxygen Monitor [Topac; 231 CJC Hwy, Suite 103 Cohasset MA 02025; 781-740-8778 F781-740-8779 topac.com sales@topa
Electronics Forum | Mon Jul 28 16:48:54 EDT 2008 | pcbbuilders
my oven has a built in profiler, it works fairly well, but it can not predict changes. my main concern was about the time right before reflow. i know that's where the flux is activated and i was worried that i may be spending too much time at the tem
Electronics Forum | Fri Aug 01 21:10:35 EDT 2008 | leo_dektec
You can keep only the 5th zone as the reflow zone. And lower the first two zones to keep a good ramping rate. Meanwhile,please note the ting temperature in software or control panel is not the exact temperature in your PCB, you'd better get a KIC or
Electronics Forum | Mon Jul 28 14:30:22 EDT 2008 | grics
Take a look at this. Remember, these are only guidlines and can not replace any paste specs. As Real Chunks said, a profiler will be of HUGE help. We use this to determine what our top side temps are and to see if we have any problems with heat sen
Electronics Forum | Fri Jul 25 15:54:22 EDT 2008 | pcbbuilders
I am trying to optimize my reflow profile. i have a 5 zone oven. lead-free: for the 1st 3 zones, i am good, at about 150-200 deg for 150 seconds. during the 4th zone, i am at a temp of 200-220 for 50 seconds. during the 5th zone, i am at 220-245 f
Electronics Forum | Mon Jul 28 11:31:42 EDT 2008 | blnorman
Ideal situation is get a technical rep from the solder paste supplier. They know their paste better, and should be able to work out a profile based on their paste and your oven. Again, a technical rep, not the sales guy.
Electronics Forum | Mon Jul 28 13:21:50 EDT 2008 | realchunks
Do you have a Slim-Kic? You can run a profile and then do predictions from there. Very useful tool.
Electronics Forum | Mon Jul 28 14:01:05 EDT 2008 | pcbbuilders
thanks, looks like an interesting product. any idea of the cost? they don't list it on their site. not sure if i can afford it yet.