Electronics Forum | Thu Aug 31 21:15:46 EDT 2000 | Dave F
From the SMTnet Library try: http://www.merix.com/resourcecntr/papers/osp.doc http://www.merix.com/resourcecntr/papers/hasl_alt.doc http://www.itm-smt.com/articles.html * "Organic Solderability Preservatives" * "OSPs - Better Living Through Modern Ch
Electronics Forum | Tue Aug 09 12:12:57 EDT 2005 | davef
Why are you placing Kapton dots on your board prior to wave soldering? * Prevent solder from touching the hole and the area around it. [If so, why do you need to do this?] * Prevent solder from flowing up through the hole and coating portions of the
Electronics Forum | Sat Mar 25 07:23:05 EST 2006 | davef
Rob It's documented that lead doesn't leach out of landfills. So, how does Eurolanders health become affected by lead in landfilled electronic products? Isn't the potential for lead poisioning from using leaded glass greater a danger? Given that
Electronics Forum | Wed Sep 03 11:42:21 EDT 2008 | robinj
If the tarnish is really dark, it is very difficult to remove. Since it is yellowish it is only in the early stages. Replating will definitely work. I have used sulfuric acid based cleaners to remove this yellowish color. But rinse well and dry quick
Electronics Forum | Fri Dec 31 10:22:54 EST 2004 | gpaelmo
I agree that something has to be done with the lead waste but I believe that a recycling program is a better alternative to lead-free. Isn't silver more toxic? How about the venting of alternate alloy fumes, let alone the effects on operators. I say
Electronics Forum | Fri Feb 09 02:30:50 EST 2007 | Muhammad Haris
What are Resins, Solvents, Activators, and Thickening Agents in Solder Paste and what are their helpful and harmful effects? AND What are the purposes/properties and effects of Sn(Tin), Pb(Lead), Ag(Silver), Bi(Bismuth), In(Indium), Cu(Copper), Ni(
Electronics Forum | Tue Oct 05 12:46:02 EDT 2021 | emeto
From what I understand SAC305 and SAC405 are considered low silver content and have the better overall mechanical qualities compared to more silver or no silver.
Electronics Forum | Thu Aug 31 18:59:55 EDT 2000 | Brian W.
Our customers use OSP, HASL, immersion tin and immersion gold as board finishes. If I recommend a finish to the customer, it is one of the immersion finishes or OSP. Those finishes have the advantage of a flat surface to deposit paste. HASL has va
Electronics Forum | Fri Aug 02 12:01:40 EDT 2002 | johnw
interesting, not at all what we were told so yes lot's of contradictions comming from them, I have to say personally I've not beein impressed with there technical service of late, are they getting complacent I ask? it's strange they say it'll cause
Electronics Forum | Wed Sep 29 19:47:44 EDT 2021 | emeto
"For the lead free soldering of electronic assemblies, the inclusion of silver in the alloy results in better wetting compared to non-silver containing alloys and also allows for a broader process window. Silver also improves joint reliab