Electronics Forum | Fri Aug 17 11:55:31 EDT 2001 | davef
5uin. Your nickel thickness is fine. Although if you wanted to trade costs, consider giving-up nickel to 150uin thickness, while increasing the gold thickness. Gold over electroless nickel creates brittle joints because of phosphorous in the nicke
Electronics Forum | Mon Aug 27 15:06:29 EDT 2001 | davef
This otta push Wolfgang over the top ... Recommended reading G.G. Harman, Wire Bonding in Microelectronics : Materials, Processes, Reliability, and Yield, 2nd edition, McGraw-Hill Electronic Packaging and Interconnection Series, 1997. G.G. Harman, R