| | Hi, | | I just cheesed my previous attempt at this. I looked through IPC 600 and couldn't find anything relating to dimensional stability of a board with regard to stretch. I found bow and twist but nothing on size. I have a PCB that is .030"
Electronics Forum | Tue Mar 23 14:08:57 EDT 2010 | davef
You have what looks to be blisters/delamination. Use IPC-A-600F as a guideline for acceptance. Usually, we start from the opinion that blisters/delamination as a fabrication issue, even if it appears during solder processing. Often blisters/delam
Electronics Forum | Fri Jan 09 04:37:13 EST 2015 | jsolloway
Hi Jeff, We have both a MY500 (4 years) and a 600 (8 months) and were the first in the UK to have both. They work well for us, enough so that we no longer use a stencil printer. Like yourselves we are a high mix CEM we make about 500 different part
Electronics Forum | Tue Jul 27 16:08:04 EDT 1999 | Kathleen at ATL
I'm working on a prototype board that requires a 600 pin BGA. This is a metal top BGA being placed on a 11" x 17" PCB about .62" thick. The part is 1.77" square with a 50 mil pitch and 30 mil bump diameter. The bumps are located on the perime
Electronics Forum | Tue Sep 18 07:52:29 EDT 2007 | davef
Does the change from supplier to supplier as a result of: * Board definition? * Differences in processing at fabs? 3 Specification Fir Tree General Technical Specification 3a Design/Layout: * IPC-2221 * IPC-2222 3b PCB Fab: * IPC-6011 * IPC-6012 * I
Electronics Forum | Fri Apr 20 05:32:39 EDT 2001 | dougie
Hi, I've just splashed out �60 on IPC-A-600F trying to find out the formula for measuring the bow and twist of raw PCB's. Much to my dismay there are 10 lines on the subject in the whole standard. Worse still is that it tells me nothing I don't alre
Electronics Forum | Tue Jul 27 11:59:19 EDT 1999 | Wolfgang Busko
While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That would m
Electronics Forum | Mon Jun 08 13:26:59 EDT 1998 | D.Hammond
I work QA at an OEM in Alberta, Canada. I saw earlier posts on the smtnet regarding PCB haloing criteria. I am currently in a dispute with my PCB vendor over the acceptability of haloing (delamination) around plated through holes and vias on a lot of
Electronics Forum | Thu Aug 21 12:06:17 EDT 2008 | pms
Thanks for your replies. The problems do not appear on the complete lot of PCB's. I don't know the percentage at this point. I agree. It also appears to me that these PCB's are over-etched. The PCB rep say's "Yea, there's a few boards that have
Electronics Forum | Sun Nov 14 14:14:47 EST 2010 | methos1979