Electronics Forum | Wed Sep 18 06:53:05 EDT 2002 | CH
1) For solder short, pls check the paste height. Too much vol will cause short. For 15 mils use 5 mils thickness stencil if possible. Check profile preheat time to prevent hot slumpof the paste. 2) type 4 powder will be better for 15 mils pit
Electronics Forum | Tue Feb 20 18:04:53 EST 2007 | coop
I am not familiar with the YV100XG pick & place but you might want to increase the mount height of these components The double stick tape isn't as thick solder paste. it might be pushing the component too far down causing it to twist. I encountered
Electronics Forum | Tue Jul 19 08:26:46 EDT 2016 | pavel_murtishev
Aleksander, The answer is no. Solder deposit being printed is 80um-150um in height depending on PCB design what is two times higher than any track covered by solder mask. Molten solder will merely center the component. QFNs are prone to soldering
Electronics Forum | Mon Jul 18 12:24:53 EDT 2016 | oleksz
Some people involved in PCB assembly process claim that SMD components reflow soldering problems are often caused by traces running under a component. According to this claim, trace (or any copper) covered by solder mask and placed under SMD componen
Electronics Forum | Mon Jul 18 12:25:30 EDT 2016 | oleksz
Some people involved in PCB assembly process claim that SMD components reflow soldering problems are often caused by traces running under a component. According to this claim, trace (or any copper) covered by solder mask and placed under SMD componen
Electronics Forum | Tue Oct 12 22:22:34 EDT 1999 | se
| Hi, | We are in the process of evaluate our solder paste,incoming inspection over the solder paste, stencil requirments: | | 1- Is anybody using/requiring 1000 Kcps or more on viscosity to your solder paste provider ? Why ?? | 2- Is anybody using
Electronics Forum | Mon Dec 16 19:05:57 EST 2002 | davidduke
Steve , I agree with all the responses you have received. Randy Villeneuve is absolutly correct in all of his assesments and I would consider him an expert with the process , Gris is correct about adding a "heat sink" to the process complicating pr
Electronics Forum | Fri Jul 13 11:33:54 EDT 2007 | realchunks
Just starting and already responsible for product quality and machine adjustment? Wow, you poor bastard. Ok, I will assume this problem happens on the bottom side of the board with a thru-hole IC. The short occurs on the side that doesn't have the
Electronics Forum | Tue Jun 25 10:16:41 EDT 2013 | davef
Hi Ryan: I assume you mean reel ... the plastic thing that contains taped components. Tape & Reel, Reel suppliers: * Advantek advantek.com/products/packaging-reels.php * Peak International peakinternational.com/tape.html * Acrotech Southwest, Inc.
Electronics Forum | Tue Aug 09 11:14:28 EDT 2016 | cyber_wolf
•Rated Speed of 40,000 CPH •140 - 8mm Device Locations •14" x 18" Max PCB Size PCB dimensions Max: 457mm x 356mm Min: 80mm x 60mm Board Thickness: 0.3 to 4.0mm Component capacity Up to 140 types (8mm tape) Placing rate 0.09 sec./component - 40,