Pb-free wave soldering with SMD

Electronics Forum | Tue Nov 29 08:50:39 EST 2005 | pjc

Band width relates to conveyor speed to achive a 2 second contact time for Sn/Pb wave soldering. A typical conveyor speed is 150cm/min with a band width (contact band width between PCB and solder) of 5cm. Now for Pb-Free wave soldering a longer conta

PB-Free HASL and Leaded Solder

Electronics Forum | Thu May 13 16:55:51 EDT 2021 | emeto

With Pb-Free HASL you can't use Pb process for sure as the melting point of tin is so much higher than the lead paste process. SAC305 is the most popular compound, unless your assembly requires something else for a specific reason.

Pb free vapor soldering

Electronics Forum | Thu Dec 22 15:36:03 EST 2005 | CC

In general two step temperature reflow process requires minimum 40 deg C delta to be sucessful. We are not using vapor phase soldering but we have similar situation when we change to SAC lead free solder for PCB component population and secondary swe

Reflow soldering issues

Electronics Forum | Mon Feb 12 11:13:12 EST 2007 | davef

Q1. If I go to the Pb-free solder paste, is it necessary that I have to change my reflow oven OR just by changing with respect to solder paste specification, I can reach my goal? A1. It depends on your current oven. Some ovens can meet the higher t

Re: When? How and What??

Electronics Forum | Tue Aug 22 10:47:28 EDT 2000 | Dr. Ning-Cheng Lee

The European WEEE has issued a new (5th) version of its recommendations. In it they say that , on January 1st, 2004, they will review the status of the Pb-Free issue. There is currently NO DEADLINE for implementation. As far as a direct replacemen

PB-Free HASL and Leaded Solder

Electronics Forum | Thu May 20 03:45:22 EDT 2021 | jineshjpr

SAC305 Will be the best choice with minimum TAL, Maximum Soak Solder Profile. Surely your solder Joint strength also will be more reliable & This can pass any kind of reliable Tests.

Pb free vapor soldering

Electronics Forum | Thu Dec 22 12:05:37 EST 2005 | Tony

Currently we are using a 2 step vapor soldering process to manufacture our std. lead soldered parts. The first step was done with a ls240 vapor fluid and the second was done with a ls200 fluid. Using a 221 deg C sn95/Ag5 solder for the first step a

Pb soldering to Pb free finishes

Electronics Forum | Fri Oct 02 14:52:24 EDT 2009 | davef

If you know "soldering Pb free (Sac based soler) to Pb/Sn coated lands is a no-no," why would soldering with Pb/Sn to Pb-free coated lands be different? If you are going to do this, follow the advice of an earlier poster who recommended higher peak s

PB-Free HASL and Leaded Solder

Electronics Forum | Fri May 14 14:46:56 EDT 2021 | emeto

Not following the lead paste process window has a whole set of risks for joints quality and reliability.

Pb free BGA and Sn Pb solder paste

Electronics Forum | Thu May 06 06:47:12 EDT 2004 | praveen

Hi, I just need to undestand any issue? If I mount Pb free BGA and use normal SN/Pb solder paste?


pb-free and soldering searches for Companies, Equipment, Machines, Suppliers & Information

Selective Soldering Nozzles

High Precision Fluid Dispensers
Selective soldering solutions with Jade soldering machine

Benchtop Fluid Dispenser
Fully Automatic BGA Rework Station

Thermal Transfer Materials.