Electronics Forum | Fri Jun 19 14:25:24 EDT 1998 | Earl Moon
| | Has anyone had experience with placing BGA on gold plated boards. I thought I read a while ago there was a problem with embrittlment causing cracked joints. If anyone has experience with this your feedback would be great. | | Mike | There has b
Electronics Forum | Wed Dec 08 04:19:16 EST 1999 | pascal MATHIEU
I am working in electronic automotive industry and today we are facing to a very serious problem : if we want to use a PCBoard with a copper thickness of 90�m + fine pitch circuit (0.65mm, 0.5mm) the supplier(several) of the PCB has some trouble t
Electronics Forum | Sat Jun 30 11:03:29 EDT 2001 | davef
Nice to have you back on SMTnet. Some of the newer folk have missed-out on the solid contributions you�ve made to the Forum. The chicken wire cleaning basket was a classic!!! [It�s a shame that the folk at SMTnet can�t recover those files.] We bu
Electronics Forum | Tue Feb 17 04:52:13 EST 2004 | John W
There's normally a number of reasons people want to know what melts 1st, 1 - to see if you know, 2 voiding issues - whole can of worms 3 device alignment. One of our collegues has said that most balls are Eutectic, that's in fact not totally correct.
Electronics Forum | Fri May 15 21:39:48 EDT 2015 | jlawson
Reflow.. 1.Rehm (Germany) - Best in Class Best overall process stability heating system ( Alot of makers have started to copy there VX heating arrangement ). COnveyor chains can be a bit more attention in terms of maintenance on rehm , but if foll
Electronics Forum | Fri Feb 28 09:08:03 EST 2003 | davef
Without drilling through the numbers, they're probably correct. Recognize that standard warp / twist specs [IPC-A-610 1.5% for PTH only and 0.75% for SMT] are not going to make it on tech boards. You need to define specific requirements. This warp
Electronics Forum | Thu Oct 12 22:16:59 EDT 2000 | Dreamsniper
Hi Guys, I'd like to share this to all of you...you can start playing with the rests...Stated prices, if not indicated, are in Aussie $ or Singapore $. Stencil Printing Adhesive Pros a) Less Capital Equipment Cost (Short Term). In reality it is f
Electronics Forum | Wed Jun 09 02:35:10 EDT 2004 | Bernard
Base on the PORON foam rubber recommended, is it possible to apply on small BGA chip of 4x4 ball size 0.3mm. Any specific part no and supplier for this type of foam and is it a anti-static material? Would it be possible to punch out at dia. 3mm?
Electronics Forum | Wed Jan 16 07:57:58 EST 2008 | davef
Give your current supplier a shot. They probably can do a good job for you. Most wave solder pallet suppliers make SMT pallets just to stay in business.
Electronics Forum | Thu Aug 22 22:19:13 EDT 2019 | sssamw
From the picture you present, it is a pin in paste part with pin length 2.2mm (a good length for 1.6mm PCB thickness), and seems the pin tilted and touch on PCB surface, thus causes up-part. Sorry I cannot image pin tilted not before placement but i
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830