Electronics Forum | Mon Sep 09 15:38:02 EDT 2013 | arendonk
Hi, We are having issues aluminum wirebonding on ENEPIG plated PCB by a too low pull force and or having lifts (1% range). Could any body advice how to solve this problem? Is there a special wire bond grade required? How to best clean contaminant
Electronics Forum | Mon Sep 09 18:10:35 EDT 2013 | davef
I don't know, but here is a link to a paper from the fine SMTnet Technical Library on a similar topic: http://www.smtnet.com/library/files/upload/Wire-Bonding-and-Soldering-on-Enepig.pdf Contact the authors and ask for their advice and help. BR, d
Electronics Forum | Mon Jun 23 04:00:43 EDT 2003 | Paul Cooper
Hi there There are a number of things worth considering when viewing bga's. Firstly, like any other solder joint that you have been inspecting for years, suface finish is critical. Secondly, and again like other joints shape is important. Now it may
Electronics Forum | Tue Nov 07 22:44:39 EST 2017 | wrander1
Hi I'm new to the world of wire bonding. I seem to have some sort of pad contamination Preventing gold wire from bonding to aluminum pats. There appears to be a dozen microns size particles. And a slight crackling of the surface at 500 X. I am send
Electronics Forum | Tue Jul 18 16:49:49 EDT 2023 | mahasg
Hello All, I am PhD student at polytechnique Montreal. We have a CQFP44 packages and Dies of 51um pad pitch (22nm FDSOI tech) that I need to bond myself at the university using ASM Eagle Xtreme gold wire bonder in the university. we need to perform b
Electronics Forum | Fri Aug 17 11:55:31 EDT 2001 | davef
5uin. Your nickel thickness is fine. Although if you wanted to trade costs, consider giving-up nickel to 150uin thickness, while increasing the gold thickness. Gold over electroless nickel creates brittle joints because of phosphorous in the nicke
Electronics Forum | Fri Aug 17 01:40:55 EDT 2001 | V.RAMANAND KINI
We are in the watch & clock Business. We have a Watch IC chip that has to be wirebonded using Ultrasonic aluminium wedge bonder. The wire dia is 1.25mil. The PCB is made of G10 Glass epoxy copper clad laminate. The copper thickness is 18 microns. The
Electronics Forum | Mon Aug 27 15:06:29 EDT 2001 | davef
This otta push Wolfgang over the top ... Recommended reading G.G. Harman, Wire Bonding in Microelectronics : Materials, Processes, Reliability, and Yield, 2nd edition, McGraw-Hill Electronic Packaging and Interconnection Series, 1997. G.G. Harman, R
Electronics Forum | Tue Aug 21 22:24:36 EDT 2001 | davef
Root around here http://www.kns.com/resources/library/lib-wirebonding.asp
Electronics Forum | Wed Dec 29 05:58:04 EST 2021 | sophyluo1985
According to the normal theory and the feedback of our other customers, maintenance is divided into 4 ways. (Depending on the environment of your production workshop, the work head is generally inspected monthly) 1. Daily maintenance: Clean the surfa
Our Company handle AOI (Auto Optical Inspection) and SPI (Solder Paste Inspection) Machines.
Equipment Dealer / Broker / Auctions
Hwaseong-si, Gyeonggi-do, Korea
Hwaseong-si, South Korea
Phone: +82-1029254936