Electronics Forum | Wed May 04 11:54:29 EDT 2005 | HOSS
Rob, Are you hinting that the lead content of this component with dipped tin/lead solder would not be an issue with RoHS? If so, our understanding is that the legislation requires that the 6 banned substances cannot exist at greater than X% in any
Electronics Forum | Thu May 05 09:50:29 EDT 2005 | patrickbruneel
Hi Hannu, You just gave a very realistic and practical view of the lead-free dilemma. The main reason that your coil coating doesn't get removed is because of the inability of lead free alloys to wet the surface and conduct the heat. Higher temperat
Electronics Forum | Tue Jun 22 22:18:02 EDT 1999 | armin
Hi Graham, can u send me some conformal coating guidelines. i'm also interested ! my e-mail add is armin.tan@setec.com.au thanks | | Could anyone please give me any information or obtainable references concerning proper guidelines for the applica
Electronics Forum | Fri Oct 29 17:44:13 EDT 2004 | davidcb
Davef, thanks for inputs. I think your correct, we have since obtained some ionic analysis and sure enough there is relatively high chlorides on the bare pcbs. The toluene is controlled within dip tank / drying system, almost no exposure to workers.
Electronics Forum | Thu Nov 23 23:59:25 EST 2000 | terry sun
Hello to all out there, We're considering CC process,and would like to know some defferences between SSC3 of Electrolube and Humiseal 1B73, yes,I know that SSC3 is silicone one,and Humiseal 1B73 is solvent based acrylic as well as other basic propert
Electronics Forum | Thu Feb 23 16:31:09 EST 2012 | hegemon
Could be as simple as a pail full of UR coating and some wire hangars! Conformal coating is brushed on, sprayed on, and parts are dipped too, not to mention the wonderful vacuum process that is paralene. Gotta have a little more info as to your a
Electronics Forum | Wed Apr 14 17:13:08 EDT 1999 | Stephen Oltmann
| I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are consid
Electronics Forum | Wed Apr 14 17:14:49 EDT 1999 | Stephen Oltmann
Check with BTU. They have dryers in the length you need. Good luck! | | I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches
Electronics Forum | Sat Apr 17 11:56:04 EDT 1999 | Graham Naisbitt
Mike First, you MUST make sure the oven used is extracted. The coating will contain TDI. This is not nice. You would be better considering a silicone solventless. Try contacting HumiSeal. They had a material on the TAC line at Nepcon West that lo
Electronics Forum | Wed Apr 14 20:39:02 EDT 1999 | Dave F
| I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are consid