Hitachy QFP 256 leads problems

Electronics Forum | Sun Mar 18 23:01:11 EDT 2007 | diesel_1t

Hi there, I want help on the following issue. Where I work, we place a component QFP 256 terminals (20 mil pitch)from hitachi (renesas), we use a MPM UP-3000 screen printer, IP-III placement machine and Vitronics 8 zones reflow Oven. lead plating

Wetting Issues - Humidity Related

Electronics Forum | Mon May 09 16:44:33 EDT 2011 | dcell_1t

Hi, We have been struggling with an issue of non wetting on a QFP (Renesas - 256, Sn90Pb10) but the issue "desapears" sometimes for a while and then back again suddenly. This is the scenario: Component: QFP 256 / Renesas / Sn90Pb10 / 0.5 mm pitch S

0402 tombstoning and dewetting on QFP256 trade-off

Electronics Forum | Thu Mar 05 11:53:09 EST 2009 | dcell_1t

Hello to all. for certain time, we have been struggling with some issues on a PCB where have tombstoning on 0402 components (due to pad design) and dewetting in qfp256 0.5 mil pitch (discussed on another threads on this forum) component, we have pro