Electronics Forum | Mon Sep 23 18:11:10 EDT 2002 | steveb
On an assembly reflowed in air saw the same thing: 0201's with a grainular solder joint, but 0402's and above with perfectly formed joints. Reflow profile all within acceptable tolerances. Reflowing in nitrogen solves this problem, but increases t
Electronics Forum | Fri Nov 03 02:32:56 EST 2006 | shivam
HI ALL, can anybody clear me what is via tenting and via pluging?? second one, if i use via in pad for an.5mm bga what care i should taken, what should be the soldermask open in top and innerlayers for via?how it will directly connect to top layer
Electronics Forum | Wed Mar 04 14:35:16 EST 2009 | clampron
Good Afternoon Everyone, I have a customer who is inquiring as to the use of a no clean solder paste on their RoHS assembly. We are currently building this with OA, cleaning and then underfilling the QFN, BGA comonents after a sucessful ICT. Does any
Electronics Forum | Tue Aug 11 17:36:44 EDT 2009 | dyoungquist
You are looking for a complete SMT assembly line plus possible X-Ray inspection and rework equipment. The 3 components of the SMT line are stencil printer, pick-n-place machine and reflow oven. How small are your components? 0603? 0402? What is the
Electronics Forum | Thu May 30 10:31:03 EDT 2002 | robbied
Hi Yannick. This is an issue that we are just recently getting into but here is some ifo that I have gathered so far. I have seen/ used 2 different rework machines. The one we have bought is a 'PACE TF2000' which was at the lower cost end of the mar
Electronics Forum | Tue Apr 03 01:37:54 EDT 2001 | philipreyes
60% 36% 0f ball area >36% Class2 Accept Reject 45% of ball diameter >45% 20.25% of ball area >20.25% Class3 Accept
Electronics Forum | Tue May 08 21:13:04 EDT 2001 | Paul
My company is a low-volume high mix contact electronic manufacturer. We are currently looking at purchasing a pick and place machine that is capable of mounting such new components as microBGA's and other CSP's at such ball pitches as 0.5mm for examp
Electronics Forum | Wed Sep 25 10:56:27 EDT 2002 | xrayhipp
Yeah, perhaps lean more towards a ramp-to-spike profile - reducing the soak time and add a littel heat to your temp above liquid. This has worked for us with water soluable paste as we are not required to use no-clean and utilizing a 6-zone oven. G
Electronics Forum | Mon Jul 08 13:49:10 EDT 2002 | msjohnston
HI, We are looking into expanding our current x-ray inspection from manually inspection one panel per lot to 100% automated inspection for all of our BGA and CSP builds. We have 100% manual inspection at the end of our SMT lines and we are consideri
Electronics Forum | Tue Jul 09 10:15:17 EDT 2002 | msjohnston
Cal, Our parent company is a FAB and they are about to release a new generation of parts. Usually the die is qualified in a simple TSOP form factor. This time the first product quals will take place in the BGA and CSP from factors rather than the t