was this hasl finish looks like it has been corroded from the inside of the hole wall looking at the shape of the break in plating
Electronics Forum | Wed Nov 23 08:43:48 EST 2022 | charles_nguyen
I am having problem with plated hole-copper spacing. I don't know if the gap between plated hole and copper can meet the capacity of PCB manufacturers. My board have 0.5oz copper weight on outer layer and distance of 0.177MM between plated hole and c
Electronics Forum | Tue Oct 27 16:22:00 EDT 2009 | davef
It's not the first thing we think of in looking at your picture. First off, the lack of copper in the region of the red oval makes us think of a plating defect. We don't expect that moisture out-gassing through the barrel wall to show-up on opposite
Electronics Forum | Tue Oct 17 03:13:10 EDT 2006 | charless
Apoligies Steve if I did not explain myself clearly. We have made the same design using the same RoHs compliant components (which I am assured by the suppliers are process temperature capable) with both lead and lead free solder. Without wishing to
Electronics Forum | Tue Mar 25 08:29:33 EDT 2014 | sara_pcb
Please refer the attached jpegs, The problem is noticed after reflow soldering followed by conventional through hole soldering. Flux used one is MIL Std. Brush cleaning in IPA is followed after each soldering step. regards, R.Saravanan
Electronics Forum | Mon May 21 17:32:23 EDT 2001 | davef
I said: "Our electronic circuit board fabricators seal the boards in moisture barrier bags [MBB]. We discontinued the use of desiccant bags in these MBB because of concerns about the desiccant releasing materials that would affect the solderability
Electronics Forum | Wed May 27 10:19:43 EDT 1998 | Jerry
We have no problems but orientation does matter. Orient with longest side of component body perpendicuar to wave. In other words the same preference as with through hole DIPS. Idea is the same as for through hole, that the surface tension will ten
Electronics Forum | Thu Feb 05 08:39:16 EST 2004 | davef
IPC-2222 - Sectional Design Standard For Printed Board For Organic Printed Boards, Table 9-3 � Plated Through Hole Diameter To Lead Diameter Relationships will give you the standard information you require.
Electronics Forum | Thu Jan 20 08:22:14 EST 2011 | padawanlinuxero
http://www.flickr.com/photos/94427924@N00/5372753378/sizes/m/in/photostream/
Electronics Forum | Wed Jan 12 20:18:14 EST 2011 | Jacki
How many % were affected? If a few,it can be caused bcoz of PCB coating. We had encountered it and PCB house replaced for faulty boards. Since then, we do test first if we hve to solder PCBs from this PCB house.
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830