Electronics Forum | Fri Aug 14 07:27:42 EDT 1998 | Earl Moon
| | Hi, can you please tell me how to make green coating and through-hole plating of PCB? Thanks! | | Xingsheng | Xingsheng: Welcome. | Bible on PCB fabrication: Printed Circuits Handbook, Clyde Coombs, McGraw-Hill | Web resources: http://www.pw
Electronics Forum | Fri Aug 14 08:59:51 EDT 1998 | Dave F
| | | Hi, can you please tell me how to make green coating and through-hole plating of PCB? Thanks! | | | Xingsheng | | Xingsheng: Welcome. | | Bible on PCB fabrication: Printed Circuits Handbook, Clyde Coombs, McGraw-Hill | | Web resources: htt
Electronics Forum | Tue Aug 31 11:57:03 EDT 2004 | Kris
Hi Any body have any issues soldering tin lead solder paste with lead free terminations ? Components are leaded devices and chip components have read the theoritical discussions on the forum, need to know if any body has seen any real issues tod
Electronics Forum | Tue Aug 09 10:01:26 EDT 2005 | pr
We have some large plated through holes, that we protect with hand placed Kapton dots before they go into the wave. Is there a better option? We are going to see if the boardhouse can put them on for us but I was curious how others are/would do this.
Electronics Forum | Wed May 24 16:47:21 EDT 2006 | patrickbruneel
Inds, It's about time that lead-free components can stand higher temps "myth" stops. The only difference is the plating, the component itself has not changed. Can you give us an update on this threat? If you�re the same inds http://www.smtnet.com//
Electronics Forum | Fri Jun 08 18:27:03 EDT 2007 | jmelson
This is probably an inner plated layer of the component that did not bond well. It may be a component that either has the wrong surface finish for lead-free or can't handle the temperatures. Many times I have seen a similar-looking layer when the l
Electronics Forum | Fri Jul 24 07:43:56 EDT 2009 | davef
Your customer is correct. You are doing something wrong in your hand soldering process. Solder balls are a process indicator. Areas to assess are: * Moisture content of the bare board * Thickness of the copper plating in the through holes * Temperatu
Electronics Forum | Fri Sep 25 13:09:42 EDT 2009 | rmitchell
Thanks to those that responded. I eliminated the light curtain problem. The metal plate the light curtain pcb bolts to was bent. I had it aligned in our machine shop and it worked properly. I forgot to mention the error was pooping up with no fee
Electronics Forum | Tue Aug 02 10:46:03 EDT 2016 | proceng1
We are getting more and more customers wanting LED boards built on White Solder Mask. Well our printers do not get as much contrast between the white mask and the plated fiducial pad, and often the camera only sees white. Other than playing with
Electronics Forum | Wed Jan 30 03:20:00 EST 2019 | bane016
We measure each first board before the oven after every chageover...Assembling one offset and measure component, after we clear plate...We have reason why do that...But we're wasting a lot of time.So I wanted to see how you do it. Thank you for answe