Electronics Forum | Sat Oct 04 00:21:00 EDT 2003 | Dean
It would help to run a carbon, anion, cation, mixed-bed configuration with pure DI as the final rinse. IF your incomming water is really bad you can run a RO unit to "prepare" the water for ion exchange. Do you run omega meter or ionograph testing
Electronics Forum | Fri Jul 30 14:53:01 EDT 1999 | Tom B.
Hello Netters, I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinned on exposed
Electronics Forum | Fri Jul 30 17:16:59 EDT 1999 | Dave F
| Hello Netters, | | I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinned on e
Electronics Forum | Thu Sep 28 16:25:20 EDT 2023 | SMTA-72837649
I've been looking for information on how, if at all, any of you treat water after a pcb batch wash. In particular, we have a Trident LD machine, using Zestron cleaning chemical. We have a carbon tank and two mixed bed media tanks as well as two 5 mic
Electronics Forum | Mon Aug 31 21:47:56 EDT 2009 | davef
In response to your question: 3 Saponifier / non saponifier 3a Saponifiers: * Aqueous Technologies: PCB-Wash http://www.aqueoustech.com * Kyzen: XJN http://www.kyzen.com * EnviroSense: Enviro Gold #816 http://www.envirosense-inc.com 3b Non-Sapo
Electronics Forum | Mon Apr 07 04:33:43 EDT 2003 | Neil
Iman, How long after washing the boards do you process them? Are there any vias or Micro vias on any of the pads you see the blow holes on? A possible cause of a blow hole in a solder fillet or PCB is the escaping of Moisture under extreme temps. Th
Electronics Forum | Fri Jul 30 17:24:24 EDT 1999 | Dave F
| | Hello Netters, | | | | I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinne
Electronics Forum | Thu Aug 05 19:10:53 EDT 2004 | celldude
wash->ssd top->wash->sticky flux bottom side->place smt components->reflow->wash->sticky flux top side->place topside smt components->reflow->wash) ssd is basically the process of applying solder paste to the pcb with a stencil and the solder reflowe
Electronics Forum | Wed Feb 11 14:55:52 EST 2015 | erezah
we received assembled PCBs with spots that look like a bleach spots all over the PS and CS . The board house said that this is normal due to flux aqueous wash process. Can it cause problems (e.g. corrosion ) in the long run or cause issues when wor
Electronics Forum | Thu Apr 22 10:57:20 EDT 1999 | Jack Coia
On various PCB's after building processes,such as reflow, flowsolder and wash. The soldermask on the PCB's have become discoloured, like a 'marble' effect all along the solder side of the board, it is lighter in contrast than normal, although when ot
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830