Electronics Forum: white residue problems with ipa cleaning (Page 8 of 16)

Whitish Solder Joint

Electronics Forum | Fri Apr 04 09:28:59 EST 2003 | davef

Q1: Anyone has any ideas on how this post-SMT reflow solder joint could have changed to whitish joint? A1: Dunno. You need to tell us more. For instance: * What is the appearance of this white residue? [eg, glassy / coarse, milky colored / opaque,

Corrosion

Electronics Forum | Tue Oct 07 01:02:25 EDT 2003 | Hoss

Adam, I can't disagree with Pete that an Ionic contamination test may ID the affected boards. However, if you have a large number of boards to test, this may not be the answer. Omegameter testing takes 10-15 minutes per unit if memory serves. On

White Residue / Vapor Degrease

Electronics Forum | Thu Jan 14 22:59:08 EST 1999 | Chris G.

I get white residue on my PCBs after vapor degreasing. No comments on the vapor degreaser. Yes, I still use one of these. I use a vapor degreaser and a 1,1,1 replacement solvent due to the quick clean and quick dry times. Anyway, I only get white

No Clean

Electronics Forum | Tue Jun 12 18:06:17 EDT 2001 | davef

The criterion you use will depend on the test method you select. For minimum requirements, look at J-STD-001C, Para 8, "Cleanliness Requirements". I figure that you�d measure the residues on a lot of your current product, measure the res on a lot o

Re: no clean rework

Electronics Forum | Wed Aug 18 15:52:21 EDT 1999 | DENNIS FOWLER

| | | Gian | | | | | | You alarm me when you talk of white residues in a "no-clean" process. This should not happen. It sounds like you have compatibility problems between different residues and/or a poorly polymerised solder mask. | | | | | | Ther

Necessity of ROSE in commercial quality processes

Electronics Forum | Mon Feb 27 17:08:15 EST 2006 | GS

3,5 ugr/cm2 NaCl) or power components, or Raw PCB. Nothing with the solder process or fluxes. Ion Chromatography analysis was necessary to help understanding of contamination origin. When occasionally we run TIC on a NC assembled PBA (Paste ROL0 or

Necessity of ROSE in commercial quality processes

Electronics Forum | Sun Feb 26 17:40:35 EST 2006 | GS

Hi, just my comment, theoretically No Clean means no Ion Contaminants from Flux, but it some some case ion contamination (Cl-Br-F) could come out from raw PCBs, from Components, from fingerprints, etc. To incorporate a ROSE step in the pro

Re: White Residue / Vapor Degrease

Electronics Forum | Wed Jan 20 21:25:32 EST 1999 | Tony A

| I get white residue on my PCBs after vapor degreasing. No comments on the vapor degreaser. Yes, I still use one of these. I use a vapor degreaser and a 1,1,1 replacement solvent due to the quick clean and quick dry times. Anyway, I only get whi

No-Clean Wave Flux - Water Wash

Electronics Forum | Mon Mar 29 11:49:44 EST 2004 | gregoryyork

White residue, probably nothing to do with the flux but was more than likely mineral salts from resist cure problem that are only soluble in Mineral Acids. No residue is the best IF resist is good, if resist issue's use low solids Rosin No Clean and

Cleaning a No Clean

Electronics Forum | Fri Jan 14 12:20:12 EST 2011 | SheanDalton

There is a lot of information available about cleaning no-cleans. Takes chemical, mechanical and thermal energy. Find the right chemistry for the flux (not something like IPA that will most likely just smear the residues around and cause problems


white residue problems with ipa cleaning searches for Companies, Equipment, Machines, Suppliers & Information

Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes

World's Best Reflow Oven Customizable for Unique Applications
Electronic Solutions

Wave Soldering 101 Training Course
design with ease with Win Source obselete parts and supplies

Thermal Transfer Materials.